A solid fertilizer, humic acid technology, applied in organic fertilizers, fertilizer mixtures, fertilization devices and other directions, can solve the problems of lack of modern production technology and scale, backward production technology, high energy consumption, and achieve improved crop quality and no environmental pollution. , the effect of saving energy
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] 1. Preparation of active weathered coal containing active humic acid
[0019] Weigh the following materials into the activation reaction tank:
[0020] (1) Water (tap water or underground well water) 35kg, water temperature 20°C;
[0021] (2)K 2 CO 3 (content 98.5%) 4.5kg;
[0022] (3) 50kg of weathered coal (from Huolinhe Coal Mine, HA content is 60.1%, particle size is above 60 mesh):
[0023] Under the condition that stirring speed is 50 rev / mins, after above-mentioned material is stirred for 15 minutes, add hydrogen peroxide 5kg (its weight percent composition is 29%) in activation reaction tank again, rise to stirring speed to be 200 rev / mins simultaneously Separate, react at 27°C for about 5 minutes, after the material forms a porous bulk, pour it on the drying field to dry naturally, pulverize, and sieve (20 mesh), that is, active weathering with uniform particle active humic acid content of 61.3%. coal.
[0024] 2. Preparation of humic acid solid fertilize...
Embodiment 2
[0037] Embodiment 2 Preparation of active weathered coal containing active humic acid
[0038] Put 50Kg of weathered coal with a particle size of 100 mesh and a humic acid content of 50% in an activation reaction tank, start stirring at a speed of 50 rpm, and add 40Kg of water and 4.5Kg of K 2 CO 3 , after stirring for 20 minutes, add 7Kg H 2 o 2 At the same time, increase the stirring speed to 300 rpm, and react at 35°C for 5 minutes, and the reaction product is naturally aired for 8 hours. After drying, it is slightly rolled and sieved (20 mesh), and the active weathered coal with uniform particles is formed. . The weight percentage of active humic acid is 80.60% after testing.
Embodiment 3
[0039] Embodiment 3 Preparation of active weathered coal containing active humic acid
[0040] Put 50Kg of weathered coal with a particle size of 100 mesh and a humic acid content of 50% in an activation reaction tank, start stirring at a speed of 50 rpm, and add 30Kg of water and 3.5Kg of Na 2 CO 3 , 2KgNH 4 HCO 3 , after stirring for 20 minutes, add 1Kg potassium percarbonate and 4Kg H 2 o 2 At the same time, the stirring speed was increased to 500 rev / min, and reacted for 5 minutes at 25°C to form a bulky body. The reactant was poured out and moved to the drying field. After natural drying for 5 hours, it was slightly rolled and sieved (20 mesh), that is, to form active weathered coal with uniform particles. The weight percentage of active humic acid is 74.0% after testing.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com