[0015] Mix 50g of lutein (content: 70% ± 5%) and 25g of microporous starch at room temperature, add 35g of maltodextrin, 6g of CMC-Na (carboxymethyl cellulose), 5g of sucrose, tert-butyl Mix 0.1g of phenol and 15g of silk fibroin colloid in aqueous solution, stir evenly, grind evenly with a colloid mill, spray dry the colloid at an inlet air temperature of 150°C, and control the outlet air temperature at 80°C to 90°C. Microcapsules with an average particle size of 150 μm and a lutein content of 22% were obtained.
Embodiment 2
[0017] Mix 50g of lutein (content: 70%±5%) and 20g of cross-linked microporous starch at room temperature, add 40g of cyclodextrin, 3g of hydroxyethyl cellulose, 5g of lactose, 0.1g of vitamin C, and gum arabic Mix the aqueous solution of 20g colloid, stir evenly, and use a high-pressure homogenizer to homogenize evenly. The colloid is spray-dried at the inlet air temperature of 150°C, and the outlet air temperature is controlled at 80°C to 90°C. Microcapsules with an average particle size of 121 μm and a lutein content of 21% were obtained.
Embodiment 3
[0019] Mix 50g of lutein (70%±5%) with 25g of microporous starch at room temperature, add 40g of maltodextrin, 6g of hydroxypropyl methylcellulose, 5g of glucose, 0.1g of vitamin E, and xanthan gum Mix the aqueous solution of 15g colloid, stir evenly, grind evenly with a colloid mill, spray dry the colloid at the inlet air temperature of 150°C, and control the outlet air temperature at 80°C to 90°C. Microcapsules with an average particle size of 132 μm and a lutein content of 21% were obtained.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com