[0053]Produce concentrated liquid raw material ratio of the present invention: potassium permanganate 10kg, potassium perchlorate 50kg, sodium nitrate 50kg, potassium dichromate 10kg, boron oxide 20kg, borax 10kg, sodium chloride 100kg, rare earth chloride 10kg, water 740kg, put Put into a shearing machine with a rotating speed of 1800 rpm, and stir; then 15kg of calcium carbonate, 5kg of calcium oxide, and 5kg of magnesium carbonate are respectively pulverized into powders with a particle size of less than 1mm, mixed, and 75kg of water is added, stirred evenly, and then mixed with the above Agents were mixed and stirred for 1 hour to obtain the concentrated solution of the present invention. When spraying on coal, take 5kg of energy-saving, sulfur-reducing and dust-removing concentrate and dilute it with 200kg of water, spray it on 5000kg of coal, and test it on a 10T / hour chain boiler. The temperature of the furnace is increased by 121°C, which can reduce the smoke and dust b...
example 2
[0055] Produce concentrated liquid raw material proportioning of the present invention: potassium permanganate 15kg, potassium perchlorate 50kg, sodium nitrate 50kg, potassium dichromate 10kg, boron oxide 15kg, borax 5kg, sodium chloride 130kg, rare earth chloride 5kg, water 730kg, put Put into a shearing machine with a rotating speed of 1800 rpm, and stir; then 15kg of calcium carbonate, 15kg of calcium oxide, and 10kg of magnesium carbonate, respectively pulverized into powders with a particle size of less than 1mm, are mixed, and 65kg of water is added, stirred evenly, and then mixed with the above The solution was mixed and stirred for 1 hour to obtain the concentrated solution of the present invention. When spraying coal, take 5kg of energy-saving, sulfur-reducing and dust-removing concentrated solution, dilute it with 200kg of water, spray it on 5000kg of coal, and test it on a 35T / hour coal throwing furnace. The temperature of the furnace is increased by 138°C, which can...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com