Alcohol fuel additive capable of preventing metal corrosion and inhibiting rubber swelling
A technology for rubber swelling and metal corrosion, applied in the field of alcohol fuel additives, can solve problems such as metal corrosion, and achieve the effect of inhibiting metal corrosion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0056] The preparation method of the present invention: under normal temperature and normal pressure, the required components are respectively added into the mixer according to their volume parts through a flow pump; through thorough mixing, the desired inhibitor is obtained.
[0057] The polar group of the additive involved in the present invention is adsorbed on the surface of metals such as copper and aluminum, and the non-polar long chain forms a protective film on the metal surface to prevent the electrochemical corrosion of the metal by ions, and the protective film formed on the metal surface is also weakened. It prevents the corrosion of active sulfur in methanol fuel; some functional groups in the compound form complexes with certain strength with active materials such as Fe, and form a dense coating layer on the surface of steel to prevent alcohol gasoline from corroding active metals. At the same time, due to the addition of the rubber plasticizer, the swelling of th...
specific Embodiment approach 1
[0063] Under normal temperature, normal pressure, fireproof, explosion-proof, and static-free environment, proceed as follows:
[0064] (1) according to the volume portion of the present invention, be modulated into alcohol fuel additive;
[0065] (2) The additive and high-proportion methanol fuel, such as M85 and M100, are fully reconciled according to the volume ratio of 1 to 2:99 to 98, and a high-proportion methanol fuel with corrosion inhibition and swelling resistance can be obtained;
specific Embodiment approach 2
[0067] Under normal temperature, normal pressure, fireproof, explosion-proof, and static-free environment, proceed as follows:
[0068] (1) according to the ratio of the present invention, adjust the alcohol fuel additive;
[0069] (2) fully reconcile the added additive with the denatured methanol that does not have the anti-corrosion and swelling effect according to the volume ratio of 0.5~1:99.5~99;
[0070] (3) Fully mix the denatured fuel methanol prepared in step (2) with gasoline according to the required volume ratio, and then M5-M50 methanol gasoline can be prepared.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com