A bio-liquid and fuel technology, applied in the liquid carbon-containing fuel, fuel, petroleum industry and other directions, can solve the problem of inability to solve the problem of carbon deposition, and achieve the effects of easy purchase of raw materials, simple production process, and sufficient combustion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Example Embodiment
[0033] Example 1:
[0034] Place each raw material in the reaction kettle in the following weight ratio:
[0035] Alkyl alcohol amide 2%, potassium hydroxide 1%, fatty alcohol 3%, methanol 72%, ethanol 10%, additives 12% (among which, ferrocene 1%, toluene 2%, hydrogen peroxide 9%).
[0036] The raw materials in the reactor are heated to 35°C, aerodynamically stirred for 20 minutes, and allowed to stand at room temperature for more than 2 hours, and then filtered to obtain a special fuel for the kitchen instead of liquefied gas.
[0037] The comparison data of the use of the special fuel for the kitchen and the liquefied gas prepared according to the method of this embodiment 1:
[0038] Serial number
[0039] 7
Example Embodiment
[0040] Example 2:
[0041] Place each raw material in the reaction kettle in the following weight ratio:
[0042] Alkyl alcohol amide 1%, potassium hydroxide 0.5%, fatty alcohol 2%, methanol 80%, ethanol 8%, additives 8.5% (of which, ferrocene 0.5%, toluene 2%, hydrogen peroxide 6%).
[0043] The raw materials in the reactor are heated to 35°C, aerodynamically stirred for 20 minutes, and allowed to stand at room temperature for more than 2 hours, and then filtered to obtain polymerized bio-liquid fuel.
Example Embodiment
[0044] Example 3:
[0045] Place each raw material in the reaction kettle in the following weight ratio:
[0046] Alkyl alcohol amide 2%, potassium hydroxide 1.5%, fatty alcohol 5%, methanol 60%, ethanol 15%, additives 16.5% (of which, ferrocene 1.5%, toluene 5%, hydrogen peroxide 10%).
[0047] The raw materials in the reaction kettle are heated to 35°C, aerodynamically stirred for 20 minutes, and allowed to stand at room temperature for more than 2 hours, and then filtered to obtain an alternative polymerized biological liquid fuel.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap