Elastic colorized printing paste and production method thereof
A printing paste and elasticity technology, applied in dyeing method, textile and papermaking, etc., can solve the problems of non-ideal use effect and no published technical materials, etc., and achieve the effect of improving gloss, good elasticity and operation control.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] (1) Emulsification: Add 20 grams of itaconic acid, 350 grams of ethyl acrylate, 71 grams of allyl polyoxyalkyl epoxy ether, and γ-methacryloyloxypropyltrimethoxysilane to a stainless steel kettle. 10 grams, 42 grams of methyl methacrylate, 2 grams of fatty alcohol polyoxyethylene ether XL-90, 550 grams of deionized water, stirred and emulsified for 20 minutes to prepare an emulsion.
[0020] (2) Initiate polymerization reaction: get 20% of the total amount of emulsion, namely 209 grams, add in the reactor, be warming up to 80-82 ° C, add the mixed solution of 1.27 grams of initiator ammonium persulfate and 50 grams of water, initiate, in At this temperature, the remaining 836 grams of the emulsion was added dropwise, and the mixed solution of 0.63 grams of ammonium persulfate and 50 grams of water was added dropwise, and the dropwise addition was completed in 1-2 hours. -40℃, adjust the pH to 7±0.5 with ammonia water;
[0021] (3) Compounding: Add 300-310 grams of supe...
Embodiment 2
[0023] The weight ratio of raw materials is: 20.5 grams of itaconic acid, 355 grams of ethyl acrylate, 72 grams of allyl polyoxyalkyl epoxy ether, 10.5 grams of γ-methacryloyloxypropyl trimethoxysilane, methyl methacrylate 43 grams of methyl methacrylate, 2.1 grams of fatty alcohol polyoxyethylene ether XL-90, 2.1 grams of ammonium persulfate, 580 grams of deionized water, and 310 grams of ultrafine aluminum silicate. The production process is the same as in Example 1.
Embodiment 3
[0025] The weight ratio of raw materials is: 21 grams of itaconic acid, 360 grams of ethyl acrylate, 73 grams of allyl polyoxyalkyl epoxy ether, 10.5 grams of γ-methacryloyloxypropyl trimethoxysilane, methyl methacrylate 4 grams of methyl methacrylate, 2.1 grams of fatty alcohol polyoxyethylene ether XL-90, 2.1 grams of ammonium persulfate, 600 grams of deionized water, 310 grams of ultrafine aluminum silicate, and the production process is the same as in Example 1.
[0026] The using method of the elastic color printing paste of the present invention:
[0027] Take this product and add the required paint paste, stir it evenly, and then it can be used for printing.
[0028] This product (hereinafter referred to as FS-412R) is compared with the representative similar products on the market: Ning Bodi KE product and domestic DR-301 product:
[0029] Product name
project
FS-412R
KE
DR-301
Exterior
white paste ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.