Light-color quenching oil complexing agent composition and preparation method thereof
A technology of quenching oil and compounding agent, applied in the direction of quenching agent, manufacturing tools, heat treatment equipment, etc., to achieve the effect of excellent high-temperature cooling performance, good cooling performance, and excellent rust-proof performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Add 8 parts of polyisobutene with a molecular weight of 30,000 to 50,000, 12 parts of polyisobutene with a low molecular weight of 950 to 3400, and 20 parts of barium sulfonate petroleum sulfonate T701 into the reactor and raise the temperature to 80°C. After it dissolves, Then add 10 parts of imidazoline oleate, 9 parts of 2,6-di-tert-butyl-p-cresol T501, 6 parts of alkyl diphenylamine ADPA-98, 35 parts of polyisobutylene bis-succinimide T154, and stir for 2 hours , After filtering, it is the finished product. Take 4 parts of the finished product and dilute 96 parts of base oil for use. The base oil is 150SN or 75SN.
Embodiment 2
[0020] Add 10 parts of polyisobutene with a molecular weight of 30,000 to 50,000, 15 parts of polyisobutene with a low molecular weight of 950 to 3400, and 25 parts of barium sulfonate petroleum sulfonate T701 into the reactor and raise the temperature to 90°C. After it dissolves, Then add 5 parts of imidazoline oleate, 3 parts of 2,6-di-tert-butyl-p-cresol T501, 2 parts of alkyl diphenylamine ADPA-98, 40 parts of polyisobutylene bis-succinimide T154, and stir for 2.5 hours , After filtering, it is the finished product, and then take 6 parts of the finished product and dilute 92 parts of base oil for use. The base oil is 150SN or 75SN.
Embodiment 3
[0022] Add 17.6 parts of polyisobutene with a molecular weight of 30,000 to 50,000, 26.4% of polyisobutene with a low molecular weight of 950 to 3400, and 44 parts of barium sulfonate petroleum sulfonate T701 into the reactor and raise the temperature to 100°C. After it dissolves, Then add 1 part of imidazoline oleate, 0.6 part of 2,6-di-tert-butyl-p-cresol T501, 0.4 part of alkyl diphenylamine ADPA-98, 10 parts of polyisobutylene bis-succinimide T154, and stir for 3 hours , after filtering, be the finished product of the present invention, get 8 parts of finished product again, can use after 92 parts of base oil dilutions, and base oil adopts 150SN or 75SN.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com