Embodiment 1
[0020] A kind of solid watercolor pigment, based on the total weight of the watercolor pigment, its raw material formula is: 20 parts of gum arabic, 25 parts of polyethylene glycol 6000, 6 parts of white lake essence, 5 parts of glycerin, 30 parts of calcium carbonate, 5 parts of kaolin 1 part, 7 parts of titanium dioxide, 0.8 part of polycarboxylate sodium salt dispersant, 1 part of nonionic wetting agent and 0.2 part of antifungal agent. The pigment is prepared into blocks by the following steps:
[0021] (1), take each raw material in proportion;
[0022] (2) Preheat the airtight kneader and screw extruder, put all the powder raw materials into the airtight kneader, use the pulverizer to pre-mix and disperse the powder raw materials, then add the liquid raw materials, after fully stirring, heat to 75 ° C, pass Screw extruder extrusion molding;
[0023] (3), cooling the extrudate of step (2) to make it harden, and cutting into blocks to obtain block-shaped watercolor paint...
Embodiment 2
[0026] A kind of solid watercolor pigment, based on the total weight of the watercolor pigment, its raw material formula is: 18 parts of gum arabic, 28 parts of polyethylene glycol 8000, 5 parts of glycerin, 30 parts of calcium carbonate, 5 parts of kaolin, 12 parts of fast red 1.8 parts, 1.8 parts of polycarboxylate sodium salt type dispersant and 0.2 parts of antifungal agent. According to the method identical with embodiment 1, make block watercolor paint.
[0027] Watercolor pigments have been tested: fineness ≥ grade 8 (10 parts aqueous solution, GB / 1724-79); average density 1.80g / cm 3 , water absorption < 1 part (24 hours * 25 ℃), low viscosity (the phenomenon of sticking to the box will not occur).
Embodiment 3
[0029] A kind of solid watercolor pigment, based on the total weight of the watercolor pigment, its raw material formula is: 18 parts of gum arabic, 25 parts of polyethylene glycol 8000, 7 parts of glycerin, 31 parts of calcium carbonate, 5 parts of kaolin, 15 parts of carbon black , 2 parts of polycarboxylate sodium salt type dispersant, 2 parts of nonionic wetting agent. According to the method identical with embodiment 1, make block watercolor paint.
[0030] Watercolor pigments have been tested: fineness ≥ grade 8 (10 parts of aqueous solution, GB / 1724-79); average density 1.80g / cm3, water absorption < 1 part (24 hours * 25°C), low viscosity (no sticking to on the box).
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com