Unlock instant, AI-driven research and patent intelligence for your innovation.

Phosphate leather retanning fatliquoring agent and preparation method thereof

A technology of retanning, fatliquoring and phosphate esters, applied in leather dipping, small hide/big hide/leather/fur treatment, small hide/big hide/leather skin/fur chemical treatment, etc., can solve the greasy surface of finished leather , long-term hardening, easy migration and other problems, to achieve the effect of improving absorption rate and water solubility

Inactive Publication Date: 2013-02-13
SHAANXI UNIV OF SCI & TECH
View PDF1 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, after a long time of storage, the oil is easy to migrate in the leather, so the surface of the finished leather is greasy and hard after a long time.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Phosphate leather retanning fatliquoring agent and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0024] The first step, get 98 parts of maleic anhydride, 10.8 parts of initiator benzoyl peroxide by mass parts and add in the reactor with agitator and thermometer, then add maleic anhydride and initiator total mass 3 times the organic solvent toluene, feed enough N into the reactor 2 To get rid of the oxygen in the reactor, after mixing evenly, heat up to 100°C, add 43.2 parts of 50% benzoyl peroxide aqueous solution, 104 parts of styrene and 338 parts of stearyl acrylate solution at 100°C The reaction was carried out for 6h; the whole reaction process continued to feed N 2 , to maintain the anaerobic state;

[0025] In the second step, add 200 parts of polyethylene glycol MPEG-200 to the reaction system of the first step, and react at 80° C. for 6 hours;

[0026] In the third step, control the temperature and slowly add 137 parts of phosphorylation reagent P to the product in batches at 20°C 2 o 5 (Phosphorus pentoxide), the feeding time is 1h, then the temperature is r...

Embodiment 2

[0029] The first step, get 98 parts by mass of maleic anhydride, 10.8 parts of initiator azobisisobutyronitrile and add in the reactor with stirrer and thermometer, then add maleic anhydride and initiator total mass 5 times the organic solvent N-methylformamide, feed enough N into the reactor 2 To get rid of the oxygen in the reactor, after mixing evenly, heat up to 120°C, add 43.2 parts of 50% azobisisobutyronitrile aqueous solution, 104 parts of styrene and 338 parts of octadecyl acrylate solution at the same time, at 120 ℃ for 4 hours; the whole reaction process continued to feed N 2 , to maintain the anaerobic state;

[0030] In the second step, add 500 parts of polyethylene glycol MPEG-400 to the reaction system of the first step, and react at 100° C. for 2 hours;

[0031] In the third step, control the temperature and slowly add 165 parts of phosphorylation reagent H to the product in batches at 25°C 4 P 2 o 7 (pyrophosphoric acid), the feeding time is 2h, then the ...

Embodiment 3

[0034] The first step, get 98 parts of maleic anhydride, 10.8 parts of initiator benzoyl peroxide by mass parts and add in the reactor with agitator and thermometer, then add maleic anhydride and initiator total mass 4 Times the organic solvent dimethyl sulfoxide, feed enough N into the reactor 2 To get rid of the oxygen in the reactor, after mixing evenly, heat up to 90°C, add 43.2 parts of 50% aqueous solution of azobisisobutyronitrile, 104 parts of styrene and 338 parts of stearyl acrylate solution at 90 Reaction at ℃ for 8h; the whole reaction process continued to feed N 2 , to maintain the anaerobic state;

[0035] In the second step, add 800 parts of polyethylene glycol MPEG-600 to the reaction system of the first step, and react at 95° C. for 3 hours;

[0036] In the third step, control the temperature and slowly add 150 parts of phosphorylation reagent PCl to the product in batches at 30°C 3 (Phosphorus trichloride, feed time is 1.5h, then be warming up to 70 DEG C,...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to a preparation method of a novel phosphate leather retanning fatliquoring agent, and in particular relates to a preparation method of phosphorylated polyethylene glycol branched chain type styrene-maleic anhydride-octadecyl methacrylate. Multiple functional groups such as a phosphoric ester group, a carboxyl group, a long-chain alkyl group and the like are mainly contained in the molecular structure of the product. The retanning fatliquoring agent has the effects of retanning, filling, fatliquoring and auxiliary dyeing. Simultaneously, a non-ionic ethoxyl group is used for improving the water-solubility, acid resistance and electrolysis resistance of the product. The retanning fatliquoring agent has the advantage of higher application value in leather processing.

Description

technical field [0001] The invention relates to a leather retanning and fatliquoring agent and a preparation method thereof, in particular to a phosphate ester leather retanning and fatliquoring agent and a preparation method thereof. Background technique [0002] At present, sulfated fatliquor is a kind of leather fatliquoring agent widely used in China. It has a strong fatliquoring oily feeling and is mainly adsorbed on leather fibers through physical adsorption or hydrogen bonding and other non-chemical bonding forms. But after standing for a long time, the oil is easy to migrate in the leather. Therefore, the surface of the finished leather is greasy and hard after a long time. [0003] In the 1980s, the development and application of phosphate fatliquoring agents began at home and abroad. Because phosphate ester fatliquoring agents contain active phosphate ester groups, they can interact with Cr on leather fibers. 3+ Combined with other mineral tanning agents in the fo...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C08F220/18C08F212/08C08F222/08C08F8/14C08F8/40C08G81/02C14C9/04
Inventor 强西怀张辉闫哲冯源
Owner SHAANXI UNIV OF SCI & TECH