Method for preparing autoclaved brick by using refined magnesium slags and fly ash
A technology for fly ash and autoclaved bricks is applied in the field of preparing autoclaved bricks by using magnesia slag and fly ash. The effect of mastery, simple craftsmanship
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Magnesium smelting slag, fly ash and aggregate are used as basic raw materials, and the aggregate used is crushed stone with a particle size of 2~4mm;
[0024] The activator used is gypsum;
[0025] Stir and mix magnesium smelting slag, fly ash and aggregate, wherein magnesium smelting slag accounts for 30% of the total weight of all basic raw materials, fly ash accounts for 50% of the total weight of all basic raw materials, and aggregate accounts for 30% of the total weight of all basic raw materials 20%; Add activator and water during the stirring process, wherein activator accounts for 5% of the total weight of all basic raw materials, and water accounts for 20% of the total weight of all basic raw materials. Stirring adopts a twin-shaft forced mixer with a stirring speed of 46r / min, the stirring time is 2min, and the mixed material is obtained after stirring evenly;
[0026] Put the mixed material to stand for digestion, the digestion time is 8 hours, and the dig...
Embodiment 2
[0032] Magnesium smelting slag, fly ash and aggregate are used as basic raw materials, and the aggregate used is crushed stone with a particle size of 2~4mm;
[0033] The activator that adopts is the equal mass mixture of gypsum and triethanolamine;
[0034] Stir and mix magnesium smelting slag, fly ash and aggregate, wherein magnesium smelting slag accounts for 10% of the total weight of all basic raw materials, fly ash accounts for 70% of the total weight of all basic raw materials, and aggregate accounts for 10% of the total weight of all basic raw materials. 20%; Add activator and water during the stirring process, wherein activator accounts for 0.1% of the total weight of all basic raw materials, and water accounts for 10% of the total weight of all basic raw materials. Stirring adopts a twin-shaft forced mixer with a stirring speed of 46r / min, the stirring time is 5min, and the mixed material is obtained after stirring evenly;
[0035] Put the mixed material to stand s...
Embodiment 3
[0040] Magnesium smelting slag, fly ash and aggregate are used as basic raw materials, and the aggregate used is crushed stone with a particle size of 2~4mm;
[0041] The activator used is gypsum;
[0042] Stir and mix magnesium smelting slag, fly ash and aggregate, wherein magnesium smelting slag accounts for 30% of the total weight of all basic raw materials, fly ash accounts for 60% of the total weight of all basic raw materials, and aggregate accounts for 30% of the total weight of all basic raw materials 10%; activator and water are added during the stirring process, wherein the activator accounts for 4% of the total weight of all basic raw materials, and water accounts for 15% of the total weight of all basic raw materials. The stirring adopts a twin-shaft forced mixer with a stirring speed of 46r / min, the stirring time is 3min, and the mixed material is obtained after stirring evenly;
[0043] Put the mixed material to stand still for digestion, the digestion time is ...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
compressive strength | aaaaa | aaaaa |
compressive strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com