Orange-red phosphorescent crystal material, as well as preparation method and use thereof
A crystalline material, orange-red phosphorescence technology, applied in luminescent materials, chemical instruments and methods, etc., can solve the problems of environmental pollution, high cost, harsh preparation conditions, etc., and achieve the effects of good photostability, low cost and high luminous efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
example 1
[0011] Example 1: (1) Weigh 25.0mg CuBr or CuBr 2 , 10.0mg of 2,5-bis(4-pyridine)-1,3,4-oxadiazole, 5mL of 25% ammonia water and 15mL of deionized water were added to a 30mL autoclave, and stirred at room temperature for 7h to obtain uniform mixing The solution. The mixed solution was heated at 220 °C for 35 h, then heated at 2 °C for 35 h. -1 cooled to room temperature at the cooling rate. After the reaction product was washed with water several times, red bulk crystals were obtained. The yield was calculated to be 55% based on the CuI used. Bright orange-red fluorescence can be seen under the irradiation of portable UV lamp BJRY26-4W.
[0012] (2) Weigh 55.0 mg of CuBr or CuBr 2 , 20.0mg of 2,5-bis(4-pyridine)-1,3,4-oxadiazole and 18mL of acetonitrile were added to a 40mL autoclave, and stirred at room temperature for 5h to obtain a well-mixed solution. The mixed solution was heated at 160 °C for 27 h, and then heated at 40 °C for 27 h. -1 cooled to room temperature a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com