Disinfectant cleaner and preparation method thereof
A technology of cleaning agent and formula, which is applied in the field of disinfectant cleaning agent and its preparation, and in the field of cleaning agent and its preparation, can solve the problems of high effective concentration, corrosiveness, high cost and price of high-efficiency disinfecting cleaning agent, and achieve remarkable antibacterial and decontamination effects, Stable chemical properties, good disinfection effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] The present invention is a kind of disinfectant cleaning agent, and it is made of the raw material of following parts by weight: 0.5 part of secondary octanol polyoxyethylene ether, 1 part of iodophor, 1 part of polyvinyl alcohol, 1 part of chloral hydrate, 2 parts of sodium carbonate 4 parts, 4 parts essence, 20 parts water.
[0014] A preparation method of a disinfectant cleaning agent, comprising the following steps:
[0015] A, the secondary octanol polyoxyethylene ether and iodophor of formula quantity are dissolved in aqueous solution, stir 40 minutes, be heated to 50 degree, be incubated 8 hours;
[0016] B, the polyvinyl alcohol of formula quantity, chloral hydrate and sodium carbonate were mixed, stirred for 10 minutes, poured in the solution in step A, stirred to obtain mixed solution;
[0017] C. Pour the essence of the formula into the mixed solution in step B, heat while stirring, heat to 90 degrees, keep warm for 14 hours, and cool to room temperature.
Embodiment 2
[0019] The invention is a disinfectant cleaning agent, which is made of the following raw materials in parts by weight: 2 parts of secondary octanol polyoxyethylene ether, 2 parts of iodophor, 3 parts of polyvinyl alcohol, 1.5 parts of chloral hydrate, 5 parts of sodium carbonate 6 parts, 6 parts of essence, 25 parts of water.
[0020] A preparation method of a disinfectant cleaning agent, comprising the following steps:
[0021] A, the secondary octanol polyoxyethylene ether and iodophor of formula quantity are dissolved in aqueous solution, stir 50 minutes, be heated to 70 degree, insulation 10 hours;
[0022] B, the polyvinyl alcohol of formula quantity, chloral hydrate and sodium carbonate were mixed, stirred for 15 minutes, poured in the solution in step A, stirred to obtain mixed solution;
[0023] C. Pour the essence of the formula into the mixed solution in step B, heat while stirring, heat to 90 degrees, keep warm for 14 hours, and cool to room temperature.
Embodiment 3
[0025] The present invention is a kind of disinfection cleaning agent, and it is made of the following raw materials in parts by weight: 1 part of polyoxyethylene sec-octyl alcohol, 1.5 parts of iodophor, 2 parts of polyvinyl alcohol, 1.2 parts of chloral hydrate, 4 parts of sodium carbonate 5 parts, 5 parts essence, 20 parts water.
[0026] A preparation method of a disinfectant cleaning agent, comprising the following steps:
[0027] A, the secondary octanol polyoxyethylene ether and iodophor of formula quantity are dissolved in the aqueous solution, stir 45 minutes, be heated to 60 degree, be incubated 9 hours;
[0028] B, the polyvinyl alcohol of formula quantity, chloral hydrate and sodium carbonate were mixed, stirred for 12 minutes, poured in the solution in step A, stirred to obtain mixed solution;
[0029] C. Pour the essence of the formula into the mixed solution in step B, heat while stirring, heat to 90 degrees, keep warm for 14 hours, and cool to room temperature...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com