Method for strengthening gold extraction of iron gold concentrate roasted product containing sulphur and arsenic

A calcine and iron-gold technology, applied in the field of pyro-hydro combined metallurgy, can solve problems such as harsh leaching conditions

Inactive Publication Date: 2013-04-03
CENT SOUTH UNIV
View PDF6 Cites 15 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, during the pretreatment process of oxidative roasting, the secondary wrapping of iron oxides of gold inevitably occurs. For gold concentrate calcine with high iron content, the subsequent gold extraction process is obviously hindered, and the gold leaching rate is often less than 80%. There is an urgent need to develop new methods and technologies to more fully recover gold from this type of refractory gold ore and improve resource utilization
Compared with the Chinese patent "A Method for Strengthening Acid Dissolution of Sulfur-Containing Gold Concentrate Acidified Roasting Slag", the acidic leaching of FeO is relatively easy and does not require leaching aids, but the leaching conditions are still harsh, with the acid concentration reaching 3%~40%, and Second stage acid leaching is required

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0031] Example 1: When the reduction roasting temperature is 1000°C and the roasting time is 1 hour, the metallization rate of iron reaches more than 90%. 90.80%;

Embodiment 2

[0032] Example 2: When the reduction roasting temperature is 1050°C and the roasting time is 1 hour, the metallization rate of iron reaches more than 90%. The rate is 91.27%;

Embodiment 3

[0033] Example 3: When the reduction roasting temperature is 1150°C and the roasting time is 1 hour, the metallization rate of iron reaches more than 90%. 95.84%;

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a method for strengthening gold extraction of an iron gold concentrate roasted product containing sulphur and arsenic. The high-iron gold concentrate containing sulphur and arsenic, especially high sulphur and high arsenic, hinders the subsequent chemical gold leaching process after being subjected to oxidation roasting pretreatment because of the problem that iron oxide is inevitably generated to wrap gold in a high-temperature reaction process. The invention proposes a new method for strengthening gold extraction of the iron gold concentrate roasted product containing sulphur and arsenic by a flow of 'metallized reduction roasting-acid leaching-gold leaching', namely a method for strengthening gold extraction of the iron gold concentrate roasted product containing sulphur and arsenic aiming at the problem. The method comprises the steps of firstly, carrying out metallized reduction roasting on the iron gold concentrate roasted product containing sulphur and arsenic with a reducing agent, carrying out acid leaching on the metalized roasted product, and finally carrying out chemical leaching with an acid slag. By adopting the method disclosed by the invention, the leaching rate of the iron gold concentrate roasted product containing sulphur and arsenic is higher than 95%; and important theory and technical guidance are provided for effective gold extraction of the gold roasted product.

Description

technical field [0001] The invention belongs to the field of combined pyrometallurgy and hydrometallurgy, and relates to a new method for extracting gold from sulfur-containing arsenic-iron-gold concentrate calcine, so as to realize the effective exposure of wrapped gold in the calcine, thereby producing sulfur-containing arsenic-iron-gold concentrate The efficient gold extraction of calcine creates favorable conditions. Background technique [0002] With the rapid development of the gold industry, easy-to-handle gold ores are gradually exhausted, and difficult-to-handle gold ores have gradually become the main processing resources of the gold industry. my country is relatively rich in refractory gold ore resources. Among the proven geological reserves in my country, refractory gold ore resources account for about 3 / 4 of the proven reserves, and the most typical ones are pyrite-type and arsenopyrite-type gold deposits. The proportions of pyrite and arsenopyrite in gold ore a...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C22B1/02C22B3/06C22B11/00
CPCY02P10/20
Inventor 杨永斌李骞姜涛刘晓亮郭宇峰范晓慧李光辉陈许玲张元波曾冠武刘诗倩陈利娟戈捷
Owner CENT SOUTH UNIV
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products