[0018] As shown in the accompanying drawings 1-4, a ball casting mold includes a template 1, a composite runner module 4, eight branch runner modules 5 and a hemispherical mold body 3; the composite runner module 4 is located on the template 1- In the middle of the side, eight sprue modules 5 are symmetrically mounted on both sides of the composite sprue module 4, and the angle between the axis of the sprue module 5 and the horizontal line is 15 degrees; the head of the hemispherical mold body 3 is semi-spherical , the tail end is a cylindrical positioning boss, the positioning boss of the hemispherical mold body 3 is embedded on the template 1, and is fixed by fastening screws 9, and the two sides of the template 1 are respectively provided with guide holes 2 and mounting holes 7;
[0019] The composite runner module 4 is strip-shaped, its cross section is semicircular, its upper end diameter is 70 mm, and its lower end diameter is 40 mm; the composite runner module 4 is conne...
Embodiment 2
[0022] Referring to Fig. 5, six sprue modules 5 are symmetrically mounted on both sides of the composite sprue module 4, and the angle between the axis of the sprue modules 5 and the horizontal line is 18 degrees, and the diameter of the hemispherical mold body is 100 mm.
[0023] Model plate 1 is a regular quadrilateral, and its length and width are prepared according to the requirements of the equipment modeling room. Its thickness B2 is 20 millimeters, and the thickness B1 of reinforcing plate 8 is 20 millimeters. Others are the same as in embodiment 1.
Embodiment 3
[0025] Referring to Fig. 6, four sprue modules 5 are symmetrically mounted on both sides of the composite sprue module 4, and the angle between the axis of the sprue module 5 and the horizontal line is 20 degrees, and the diameter of the hemispherical mold body is 130 mm.
[0026] Model plate 1 is a regular quadrilateral, length L and width H are prepared according to equipment requirements, its thickness B2 is 20 millimeters, and reinforcing plate 8 thickness B1 is 25 millimeters, and others are the same as embodiment 1.