A technology of phthalocyanine blue and toluene, which is applied in the direction of ink, application, organic dyes, etc., can solve the problems of serious COD emission, large consumption of raw materials, large power consumption, etc., and achieve the reduction of production cost, improvement of solvent resistance, and excellent color. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0049] Add 1000kg of crude copper phthalocyanine with purity ≥ 98.5% and free copper content ≤ 1000ppm to a 10000L horizontal ball mill, and add 30kg of copper phthalocyanine derivative shown in formula (II), turn on the ball mill for ball milling, and adjust Cooling water controls the temperature of the material in the machine at 140±2°C, and ball mills for 12 hours to obtain a ball milled product containing 30% of the α crystal form. The ball-milled product is passed through a magnetic filter to remove iron produced during ball-milling, and the product is collected to obtain an intermediate product of phthalocyanine blue 15:4, and the average particle size of the pigment is less than 1 μm. Then mix the intermediate product of phthalocyanine blue 15:4 with toluene ink, knead with a kneader and grind with a three-roller machine to obtain a special phthalocyanine blue 15:4 pigment for toluene ink.
Embodiment 2
[0051] Add 1000kg of crude copper phthalocyanine with purity ≥ 98.5% and free copper content ≤ 1000ppm to a 10000L horizontal ball mill, and add 30kg of copper phthalocyanine derivative shown in formula (II), turn on the ball mill for ball milling, and adjust Cooling water controls the temperature of the material in the machine at 145±2°C, and ball mills for 12 hours to obtain a ball milled product containing 33% of the α crystal form. The ball-milled product is passed through a magnetic filter to remove iron produced during ball-milling, and the product is collected to obtain an intermediate product of phthalocyanine blue 15:4, and the average particle size of the pigment is less than 1 μm. Then mix the intermediate product of phthalocyanine blue 15:4 with toluene ink, knead with a kneader and grind with a three-roller machine to obtain a special phthalocyanine blue 15:4 pigment for toluene ink.
Embodiment 3
[0053] Add 1000kg of crude copper phthalocyanine with purity ≥ 98.5% and free copper content ≤ 1000ppm to a 10000L horizontal ball mill, and add 30kg of copper phthalocyanine derivative shown in formula (II), turn on the ball mill for ball milling, and adjust Cooling water controls the temperature of the material in the machine at 130±2°C, and ball mills for 16 hours to obtain a ball milled product containing 35% of the α crystal form. The ball-milled product is passed through a magnetic filter to remove iron produced during ball-milling, and the product is collected to obtain an intermediate product of phthalocyanine blue 15:4, and the average particle size of the pigment is less than 1 μm. Then mix the intermediate product of phthalocyanine blue 15:4 with toluene ink, knead with a kneader and grind with a three-roller machine to obtain a special phthalocyanine blue 15:4 pigment for toluene ink.