Production method of reconstituted tobacco leaves with clean, low consumption and high filling value

A technology for reconstituting tobacco leaves and a production method, which is applied in the directions of tobacco, tobacco preparation, application, etc., can solve the problems of poor sheet bulk, difficulty in backfilling, production cost, and high maintenance cost, so as to reduce energy consumption and water consumption, and avoid a large amount of loss. , the effect of improving production efficiency

Active Publication Date: 2015-11-18
KUNMING XUBANG MACHINERY
View PDF5 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, the paper-making method tobacco sheet has the following serious defects: 1) Due to the use of paper-making technology for reference, in each link of production, especially the beating and operation links, paper-making technology pays attention to compactness and smoothness, while tobacco sheet emphasizes bulk. There is a certain contradiction, therefore, the closer the process is to the papermaking method, the worse the bulk of the produced flakes; 2) When the papermaking method is used for beating and processing, the sizing concentration can only reach 0.8-1.2%, such a low sizing concentration , when sizing, not only a large amount of sewage containing various substances must be discharged, which brings great pressure to environmental protection, but also consumes extremely high energy consumption. Each ton of sheet production requires 45-75 tons of water, 2500-3000kW of electricity, and steam consumption 10-12 tons, which is not conducive to energy saving, emission reduction, and consumption reduction; 3) The process is complicated, the equipment configuration is various, the investment is large, the land occupation is large, and the production cost and maintenance cost are high
The disadvantages of this method are: (1) The oar concentration is still lower than 1% during papermaking, so water consumption and sewage discharge are unavoidable; (2) The stalk extract needs to be concentrated, which will inevitably lead to problems such as high energy consumption and large equipment investment. ; (3) The concentrate is still coated and backfilled, so it is difficult to backfill due to the current low coating rate in the entire industry
But there are still the following deficiencies: because there is no extraction process and the modification process of the extract, its "plasticity" cannot meet the requirements of the papermaking method; because the tobacco stems are not processed in depth, the mouthfeel and tobacco taste are difficult to meet the requirements of smokers

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Production method of reconstituted tobacco leaves with clean, low consumption and high filling value
  • Production method of reconstituted tobacco leaves with clean, low consumption and high filling value

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0036] 1) After routine removal of impurities and drying, the tobacco powder is crushed into smoke powder of ≦80 mesh, and set aside;

[0037] 2) Soak the tobacco stems in hot water at 70°C at a mass ratio of 1:3, extract twice in continuous countercurrent, 40 minutes each time, and separate the solid and liquid to obtain the tobacco stem extract and residual tobacco stems;

[0038] 3) Add glycerin and calcium carbonate to the tobacco stem extract in step 2) according to the conventional amount of tobacco sheet production by the papermaking method, and mix evenly to obtain a modified tobacco stem extract;

[0039] 4) Take part of the modified tobacco stem extract in step 3), mix it with the tobacco powder in step 1) to a tobacco powder slurry with a mass concentration of 10%, and mix the rest of the modified tobacco stem extract in step 3) with step 2 ) after mixing the residual tobacco stems, beating to a coarse-stem pulp with a beating degree of 22°SR, and then finely beatin...

Embodiment 2

[0043] 1) After routine removal of impurities and drying, the shredded tobacco flakes and tobacco powder are crushed into smoke powder of ≦80 mesh for later use;

[0044] 2) Soak the tobacco stems in hot water at 45°C at a mass ratio of 1:6. First, use a conventional defibrillator to decompose the soaked tobacco stems into filaments, and then use continuous countercurrent extraction for 3 times, each time Extract for 20 minutes, and separate the solid and liquid to obtain tobacco stem extract and residual tobacco stem;

[0045] 3) Add propylene glycol, honey and calcium carbonate to the tobacco stem extract solution in step 2) according to the conventional amount of paper-making tobacco sheet production, and mix evenly to obtain a modified tobacco stem extract solution;

[0046] 4) Take part of the modified tobacco stem extract in step 3), mix it with the tobacco powder in step 1) to a tobacco powder slurry with a mass concentration of 20%, and mix the rest of the modified tob...

Embodiment 3

[0050] 1) After routine removal of impurities and drying of the broken tobacco flakes, the powder is crushed into smoke powder of ≦80 mesh and set aside;

[0051] 2) Soak the tobacco stems in hot water at 50°C at a mass ratio of 1:5, extract twice in a continuous countercurrent manner for 30 minutes each time, and separate the solid and liquid to obtain the tobacco stem extract and residual tobacco stems;

[0052] 3) Add sorbitol, honey, calcium carbonate, and pectinase to the tobacco stem extract solution in step 2) according to the conventional amount of paper-making tobacco sheet production, and mix evenly to obtain a modified tobacco stem extract solution;

[0053] 4) Take part of the modified tobacco stem extract in step 3), mix it with the tobacco powder in step 1) to a tobacco powder slurry with a mass concentration of 15%, and add conventional Wood pulp to wood fiber content is 5% mass ratio, beating to beating degree is the coarse wood pulp of 22 ° SR, then this coars...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention provides a production method of clean low-consumption high-filling-value reconstructed tobaccos. The production method comprises the following steps: with tobacco stems, broken tobacco flakes and tobacco powder generated in a cigarette product production process as main raw materials, soaking and extracting the tobacco stems, modifying an extracting solution, mixing one part of the modified extracting solution with the tobacco powder and the broken tobacco flakes to prepare tobacco powder pulp, mixing the other part of the modified extracting solution with the residual tobacco stems and beating to prepare tobacco stem fiber pulp, and performing sizing, extruding and suction filtration on the two high-concentration pulp materials to obtain stem fiber-containing tobacco sheets. According to the production method, no liquid is not discharged, so that the zero discharge is realized; tobacco substances are completely remained in the tobacco sheets; no adhesive is added, so that the tobacco sheets completely keep the original fragrance and smell of cigarettes; fibers in the tobacco stems are fully utilized, so that the basic sheet filling value is increased to be not less than 6.0cm<3> / g and finally the physical performance and quality of the tobacco sheets are improved.

Description

technical field [0001] The invention relates to a method for producing reconstituted tobacco leaves, in particular to a method for producing tobacco sheets by using tobacco waste, and belongs to the technical field of tobacco leaf processing. Background technique [0002] During the production and processing of tobacco products such as aging, compounding, leaf stem separation, shredding, drying, cooling, screening, forming and packaging, the following tobacco by-products are inevitably produced: tobacco dust, tobacco stems and fine tobacco particles, etc. For this kind of by-products, most of the existing technologies adopt the method of mixing and forming with the addition of adhesives or pulping and forming according to the papermaking process to reproduce tobacco sheets. The formula needs to reduce the tar release amount of cigarettes and reduce the harm caused by cigarettes to human body. The existing production methods of reconstituted tobacco mainly include: rolling ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): A24B3/14
Inventor 王晓耕王润哲
Owner KUNMING XUBANG MACHINERY
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products