Deoxidizing and drying agent for medical medicines and preparation method thereof
A desiccant and pharmaceutical technology, applied in the field of deoxidizing desiccant for medical drugs and its preparation, can solve the problems of few functions, short validity period, high cost, etc., and achieve the effect of reducing cost input, simple preparation process, and cheap and easy-to-obtain preparation raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0038] Formula: 35 parts of bentonite, 25 parts of attapulgite, 15 parts of bamboo charcoal powder, 5 parts of refined iron powder, 3 parts of activated manganese, 5 parts of quicklime, 0.03 part of calcium chloride and 0.1 part of calcium propionate.
[0039] Crush bentonite and attapulgite raw ore, and pass through 50-mesh screening, wind transport to the pulping equipment, stir for 3 hours and then add it to the hydraulic suspender, screen the high-quality bentonite emulsion through the overflow suspension, and enter the filter press equipment Form rods, cut into pieces with a microtome, and then bake at low temperature (250° C.) for 1 hour, and grind them into powder for later use. The prepared bentonite and attapulgite mineral powder, bamboo charcoal powder, refined iron powder, calcium chloride and calcium propionate are mixed and granulated according to the above ratio, dried and cooled under vacuum conditions, sealed and packed in vacuum.
[0040] The indicators of the...
Embodiment 2
[0043] Formula: 50 parts of bentonite, 15 parts of attapulgite, 10 parts of bamboo charcoal powder, 5 parts of refined iron powder, 3 parts of activated manganese, 8 parts of quicklime, 0.3 part of calcium chloride and 0.2 part of calcium propionate.
[0044] Crush bentonite and attapulgite raw ore, and pass through 50-mesh screening, wind transport to the pulping equipment, stir for 4 hours and then add it to the hydraulic suspender, screen the high-quality bentonite emulsion through the overflow suspension, and enter the filter press equipment Form rods, cut into slices with a microtome, then bake at a low temperature (350° C.) for 1 hour, and grind it into powder for later use. The prepared bentonite and attapulgite mineral powder, bamboo charcoal powder, refined iron powder, calcium chloride and calcium propionate are mixed and granulated according to the above ratio, dried and cooled under vacuum conditions, sealed and packed in vacuum.
[0045] The indicators of the obta...
Embodiment 3
[0048] Formula: 40 parts of bentonite, 10 parts of attapulgite, 5 parts of bamboo charcoal powder, 5 parts of refined iron powder, 3 parts of activated manganese, 10 parts of quicklime, 0.3 part of calcium chloride and 0.2 part of calcium propionate.
[0049] Crush bentonite and attapulgite raw ore, and pass through 50-mesh screening, wind transport to the pulping equipment, stir for 4 hours and then add it to the hydraulic suspender, screen the high-quality bentonite emulsion through the overflow suspension, and enter the filter press equipment Form rods, cut into slices with a microtome, then bake at a low temperature (350° C.) for 1 hour, and grind it into powder for later use. The prepared bentonite and attapulgite mineral powder, bamboo charcoal powder, refined iron powder, calcium chloride and calcium propionate are mixed and granulated according to the above ratio, dried and cooled under vacuum conditions, sealed and packed in vacuum.
[0050] The indicators of the obta...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com