Embodiment 1
[0030] A composite multi-element antiscaling and dispersing agent for mines, comprising the following components by weight:
[0031] Acrylic acid-2-acrylamide-2-methylpropanesulfonic acid copolymer 30-60 parts by weight
[0032] 2-phosphonic acid butane-1,2,4-tricarboxylic acid 30-60 parts by weight
[0033] Optional medicament 0~30 parts by weight
[0034] Among them, the optional agents are polyacrylic acid, polyepoxysuccinic acid, aminotrimethylene phosphonic acid, hydroxyethylene diphosphonic acid, aminotrimethylene phosphonic acid, sodium dodecylsulfonate, sodium dodecylsulfate, One or several kinds of sodium oleate.
[0035] In a preferred embodiment of the present invention, the following components by weight percentage are included:
[0036] Acrylic acid-2-acrylamide-2-methylpropanesulfonic acid copolymer 30~60%
[0037] 2-Phosphonic acid butane-1,2,4-tricarboxylic acid 30~60%
[0038] Optional agent 0~30%.
[0039] In a preferred embodiment of the present invent...
Embodiment 2
[0051] Mix acrylic acid-2-acrylamide-2-methylpropanesulfonic acid copolymer and 2-phosphonic acid butane-1,2,4-tricarboxylic acid in a mass ratio of 50:50; after mixing evenly, use Tap water is configured into a solution with a concentration of about 20%. After dissolving completely, stop stirring and set aside.
[0052] Add the prepared agent to the experimental water at a concentration of 10mg / L. The experiment uses mine industrial water. The scaling ion content in the water is as follows: Ca 2+ 64mg / L, Mg 2+ 50mg / L, HCO 3 - 415mg / L.
[0053] After adding the medicament, adjust the pH value of the water to 12 with calcium oxide, and after standing for 24 hours, pour out the solution, rinse the container wall with pure water 5 times, and then use the prepared hydrochloric acid to dissolve the calcium and magnesium scaling on the wall, analyze The content of calcium and magnesium is detected, and compared with the compound multi-element antiscaling dispersant for mines wit...
Embodiment 3
[0055] Mix acrylic acid-2-acrylamide-2-methylpropanesulfonic acid copolymer, 2-phosphonic acid butane-1,2,4-tricarboxylic acid, polyacrylic acid, sodium lauryl sulfate at 50:30:10 : The mass ratio of 10 is mixed evenly. After mixing evenly, use tap water to configure a solution with a concentration of about 20%, and after completely dissolving, stop stirring and set aside.
[0056] Add the prepared agent to the experimental water at a concentration of 20mg / L. The experiment uses mine industrial water. The scaling ion content in the water is as follows: Ca 2+ 64mg / L, Mg 2+ 50mg / L, HCO 3 - 415mg / L. .
[0057]After adding the medicament, adjust the pH value of the water to 11 with calcium oxide. After standing still for 24 hours, pour out the solution, rinse the container wall with pure water 5 times, and then dissolve the calcium and magnesium scaling on the wall of the container with hydrochloric acid. The content of calcium and magnesium is detected, and compared with th...
PUM
Property | Measurement | Unit |
---|---|---|
scale inhibition rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com