A Valve Surface Treatment Method Considering Both Toughness and Rigidity
A surface treatment and valve technology, applied in the field of surface treatment of valves, can solve the problems of brittleness of the spray layer, easy breakage and cracking, failure to protect the surface of the valve, etc., so as to avoid the packaging process, improve the yield and save money. cost effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] Example 1: (1), preparation of base material A: 100 parts by weight of water, 20 parts by weight of titanium dioxide, 5 parts by weight of protein, 3 parts by weight of acetone extract, 11 parts by weight of ash, 13 parts by weight of Kaolin, 27 parts by weight of wollastonite, 14 parts by weight of polyisoprene, and 18 parts by weight of dispersing aids are placed in a dispersion kettle, and then ground at a speed of 1500r / min after high-speed dispersion. Degree to 15um, obtain base material A, wherein dispersing aid comprises the defoamer that mass ratio is 0.4% and the leveling agent that mass ratio is 0.4%;
[0015] (2), preparation of base material B: 20 parts by weight of titanium dioxide, 15 parts by weight of polyvinyl chloride resin, 3 parts by weight of phosphoric acid, 10 parts by weight of benzoyl chloride compound, 7 parts by weight of calcium resin rosin, 8 parts by weight Parts by weight of bentonite, 6 parts by weight of mica powder, 4 parts by weight ...
Embodiment 2
[0019] Example 2: (1), preparation of base material A: 120 parts by weight of water, 30 parts by weight of titanium dioxide, 9 parts by weight of protein, 6 parts by weight of acetone extract, 21 parts by weight of ash, 21 parts by weight of Kaolin, 36 parts by weight of wollastonite, 25 parts by weight of polyisoprene, and 33 parts by weight of dispersing aid are placed in a dispersion kettle, and then ground at a speed of 1500r / min after high-speed dispersion. Degree to 25um, obtain base material A, wherein dispersing aid comprises the defoamer that mass ratio is 0.6% and the leveling agent that mass ratio is 0.6%;
[0020] (2), preparation of base material B: the titanium dioxide of 30 parts by weight, the polyvinyl chloride resin of 20 parts by weight, the phosphoric acid of 6 parts by weight, the benzoyl chloride compound of 15 parts by weight, the calcium resin rosin of 13 parts by weight, 11 parts by weight Parts by weight of bentonite, 15 parts by weight of mica powder...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More