An adhesive, solid wood technology, applied in the direction of adhesives, adhesive types, polyether adhesives, etc., can solve the problem of high formaldehyde emission in products, achieve simple and easy-to-obtain product raw materials, reduce free formaldehyde, increase strength and preload effect of effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] The invention is an improved solid wood adhesive, which is made from the following raw materials in parts by weight:
[0011] 2.5 parts of bisphenol epoxy resin, 2 parts of polybutadiene glycol, 1.5 parts of isomeric decanol polyoxyethylene ether, 2.5 parts of sec-octylphenol polyoxyethylene ether, 1.2 parts of dibutyltin lauryl alcohol, 0.5 parts of diglycerin 1.2 parts of alkenyl succinic acid and 2.5 parts of ethyl chrysanthemum acid.
Embodiment 2
[0013] The invention is an improved solid wood adhesive, which is made from the following raw materials in parts by weight:
[0014] 4.2 parts of bisphenol epoxy resin, 4 parts of polybutadiene glycol, 2.7 parts of isomeric decanol polyoxyethylene ether, 3.7 parts of sec-octylphenol polyoxyethylene ether, 2.3 parts of dibutyltin lauryl alcohol, 0.8 parts of diglycerin Parts, 1.8 parts of alkenyl succinic acid and 3.6 parts of ethyl chrysanthemum acid.
Embodiment 3
[0016] The invention is an improved solid wood adhesive, which is made from the following raw materials in parts by weight:
[0017] 3.8 parts of bisphenol epoxy resin, 2.4 parts of polybutadiene diol, 2.2 parts of isomeric decanol polyoxyethylene ether, 3.4 parts of sec-octylphenol polyoxyethylene ether, 1.5 parts of dibutyltin lauryl alcohol, 0.6 parts of diglycerin Parts, 1.5 parts of alkenyl succinic acid and 2.6 parts of ethyl chrysanthemum acid.
[0018] Compared with the existing products, the present invention reduces free formaldehyde, the free formaldehyde is less than 0.11, reaches E0 level, and is more environmentally friendly; the present invention has a long storage time, and the bamboo and wood products using the present invention have good water resistance and moisture resistance , the raw materials of the product are simple and easy to obtain, and are more suitable for mass production; the invention increases the strength and pre-pressing effect of the resin g...