A corrosion-type, anti-static technology, applied in the direction of conveyors, transportation and packaging, etc., can solve the problems of short service life, heat resistance, oil resistance, and unsatisfactory performance improvement of anti-static performance, so as to reduce fire hazards, Improved antistatic effect and high strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] An antistatic, oil-resistant and corrosion-resistant polyester core conveyor belt is characterized in that the components of the raw materials are composed as follows in parts by weight: 30 parts of modified neoprene rubber, 20 parts of nitrile rubber containing 30% acrylic hydrocarbon, 20 parts of trioxide Antimony, zinc borate, aluminum hydroxide are composed of 8 parts of composite flame retardant according to the mass ratio of 1:3:5, 0.6 parts of fatty acid potassium, 2 parts of zinc oxide, 1 part of stearic acid, tert-butyl peroxybenzoate 0.7 parts, accelerator TMTD 1.5 parts, polyester canvas 10 parts, carbon black 15 parts, sulfur 3 parts.
[0016] Among them, the modified chloroprene rubber is prepared by reacting 100 parts of chloroprene rubber, 25 parts of maleic anhydride, 15 parts of sulfuryl chloride and chloroform at 125° C. for 2.5 hours.
Embodiment 2
[0018] An antistatic, oil-resistant and corrosion-resistant polyester core conveyor belt is characterized in that the components of the raw materials are composed as follows in parts by weight: 33 parts of modified chloroprene rubber, 23 parts of nitrile rubber containing 30% acrylic hydrocarbon, 23 parts of di Antimony, zinc borate, aluminum hydroxide are composed of 10 parts of composite flame retardant according to the mass ratio of 1:3:5, 0.8 parts of fatty acid potassium, 3 parts of zinc oxide, 2 parts of stearic acid, tert-butyl peroxybenzoate 0.8 parts, accelerator TMTD 1.6 parts, polyester canvas 12 parts, carbon black 16 parts, sulfur 4 parts.
[0019] Among them, the modified chloroprene rubber is prepared by reacting 100 parts of chloroprene rubber, 25 parts of maleic anhydride, 15 parts of sulfuryl chloride and tetrachloroethane at 125° C. for 3 hours.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com