Plastic hot stamping foil and production method thereof
A production method and technology of hot stamping foil, applied in the field of hot stamping printing, can solve the problems of unclear pattern, insufficient brightness, intolerant of alcohol, etc., and achieve stable and continuous hot stamping processing, good hot stamping effect and good adhesion.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] The production process of a plastic hot stamping foil is: sequentially coating release material, coating coloring material, vacuum aluminum plating, and coating binder on the BOPET base film. The specific steps of the production method are as follows
[0016] 1) Preparation and coating of release material: Add 7 parts by weight of silicone modified epoxy resin, 2 parts by weight of thermoplastic acrylic resin, and 1 part by weight of Darmar resin to 28 parts by weight of mixed solvent in a stirring state In the middle, continue to stir for 30 minutes, then stop stirring, filter with a 200-mesh filter and use it on the machine; the coating speed is controlled at 130m / min, the drying temperature is 150°C, and the 220-mesh ceramic mesh roll is used for coating.
[0017] 2), preparation and coating of colorant: 3 parts by weight of colorant are added to 95 parts by weight of mixed solvent under stirring state, fully stirred for 30 minutes, then 15 parts by weight of acrylic ...
Embodiment 2
[0021] The production process of a plastic hot stamping foil is: sequentially coating release material, coating coloring material, vacuum aluminum plating, and coating binder on the BOPET base film. The specific steps of the production method are as follows
[0022] 1) Preparation and coating of release material: Add 5 parts by weight of silicone modified epoxy resin, 5 parts by weight of thermoplastic acrylic resin, and 0.5 parts by weight of Darmar resin in a stirring state to 26 parts by weight and mix In the solvent, continue to stir for 30 minutes, stop stirring, filter with a 200-mesh filter, and use it on the machine; the coating speed is controlled at 110-130m / min, the drying temperature is 135°C, and the 220-mesh ceramic mesh roller is used for coating.
[0023] 2), preparation and coating of colorant: 2 parts by weight of colorant are added to 85 parts by weight of mixed solvent under stirring state, fully stirred for 30 minutes, then 11 parts by weight of acrylic res...
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com