New material used for manufacturing light-emitting signboard and manufacturing technology thereof
A technology of luminescent signs and manufacturing techniques, applied in the field of new materials, can solve the problems of complex preparation of black and white boards, insufficient expressiveness, and high cost of use, and achieve excellent optical and various physical and chemical properties, excellent optical and various physical and chemical properties, The effect of reducing the manufacturing cost of finished products
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0066] A new material for making luminous signboards, the raw material formula of the new material is as follows:
[0067] PMMA with a molecular weight of 350,000 to 450,000 Daltons: 1kg;
[0068] Diffuser: 180~220g;
[0069] Black powder: 0.6~0.71g;
[0070] Purple powder: 0.281~0.291g;
[0071] Blue powder: 0.471~0.482g;
[0072] Dispersant: 18~23g;
[0073] UV agent: 19~27g;
[0074] Antistatic agent: 23~28g;
[0075] The black powder is carbon black powder or aniline black; the purple powder is permanent violet, quinacridone purple or cobalt violet; the blue powder is phthalocyanine blue or shihlin.
Embodiment 2
[0077] This embodiment is further optimized on the basis of the above-mentioned embodiments. In order to better realize the new material of the present invention, the following setting method is adopted in particular: the raw material formula of the new material is as follows:
[0078] PMMA 1kg with a molecular weight of 350,000-450,000 Daltons;
[0079] Diffuser: 200g;
[0080] Black powder: 0.65g;
[0081] Purple powder: 0.286g;
[0082] Blue powder: 0.475g;
[0083] Dispersant: 20g;
[0084] UV agent: 25g;
[0085] Antistatic agent: 23g.
Embodiment 3
[0087] This embodiment is further optimized on the basis of any of the above-mentioned embodiments. Further, in order to better realize the new material of the present invention, the following setting method is particularly adopted: the PMMA with a molecular weight of 350,000 to 450,000 Daltons is grainy.
PUM
Property | Measurement | Unit |
---|---|---|
glass transition temperature | aaaaa | aaaaa |
density | aaaaa | aaaaa |
boiling point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com