A post-finishing and fabric technology, applied in fiber treatment, textiles and papermaking, etc., can solve the problem of insufficient softness, and achieve the effect of softness and excellent flame retardancy

Inactive Publication Date: 2017-01-11
常熟市鑫博伟针纺织有限公司
View PDF7 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] The flame retardant, antistatic, anti-mildew, anti-moth, anti-bacterial, washable, anti-shrinkage, anti-wrinkle, and wear-resistant properties of the existing fabrics need to be improved, and the hand feeling is not soft enough

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0025] The post-finishing process of the brushed fabric comprises the following steps:

[0026] 1) 1 to 2 parts by weight of alkyl dimethyl aryl ammonium chloride, 3.1 parts by weight of dithiocarbamic acid, 4.1 parts by weight of three (hexadecanyl alcohol) ester, 1.7 parts by weight of triethanolamine stearate Ammonium salt, 0.7 parts by weight of alkyltrimethylammonium methylsulfate are dropped into 51 parts by weight of deionized water successively, and stirred evenly;

[0027] 2) Add 3.1 parts by weight of hydroxyethyl cellulose, 1.2 parts by weight of petroleum sulfonate, 0.7 parts by weight of mannan, 4.2 parts by weight of polyoxypropylene glycol, and 0.4 parts by weight of pomegranate peel powder, and continue to stir until fully Mix evenly to prepare finishing liquid;

[0028] 3) Then pad the fabric in the finishing solution, take it out and dry it at a constant temperature.

Embodiment 2

[0030] The post-finishing process of the brushed fabric comprises the following steps:

[0031] 1) 1 part by weight of alkyl dimethyl aryl ammonium chloride, 3.1 parts by weight of dithiocarbamic acid, 4.1 parts by weight of three (hexadecyl alcohol) esters, 1.7 parts by weight of triethanolamine stearate quaternary ammonium salt , 0.7 parts by weight of alkyltrimethylammonium methosulfate are dropped into 51 parts by weight of deionized water successively, and stirred evenly;

[0032] 2) Add 3.1 parts by weight of hydroxyethyl cellulose, 1.2 parts by weight of petroleum sulfonate, 0.7 parts by weight of mannan, 4.2 parts by weight of polyoxypropylene glycol, and 0.4 parts by weight of pomegranate peel powder, and continue to stir until fully Mix evenly to prepare finishing liquid;

[0033] 3) Then pad the fabric in the finishing solution, take it out and dry it at a constant temperature.

Embodiment 3

[0035] The post-finishing process of the brushed fabric comprises the following steps:

[0036] 1) 2 parts by weight of alkyl dimethyl aryl ammonium chloride, 3.1 parts by weight of dithiocarbamic acid, 4.1 parts by weight of three (hexadecyl alcohol) esters, 1.7 parts by weight of triethanolamine stearate quaternary ammonium salt , 0.7 parts by weight of alkyltrimethylammonium methosulfate are dropped into 51 parts by weight of deionized water successively, and stirred evenly;

[0037] 2) Add 3.1 parts by weight of hydroxyethyl cellulose, 1.2 parts by weight of petroleum sulfonate, 0.7 parts by weight of mannan, 4.2 parts by weight of polyoxypropylene glycol, and 0.4 parts by weight of pomegranate peel powder, and continue to stir until fully Mix evenly to prepare finishing liquid;

[0038] 3) Then pad the fabric in the finishing solution, take it out and dry it at a constant temperature.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses an after-finishing process of a brushed fabric. The after-finishing process of the brushed fabric comprises the following steps: 1) putting 1 to 2 parts by weight of alkyl dimethyl aryl ammonium chloride, 3.1 parts by weight of dithiocarbamic acid, 4.1 parts by weight of tri(hexadecenol)ester, 1.7 parts by weight of stearic acid triethanolamine ester quaternary ammonium salt and 0.7 part by weight of methylsulfuric acid alkyl trimethylammonium sequentially into 51 parts by weight of deionized water and stirring uniformly; 2) putting 3.1 parts by weight of hydroxyethyl cellulose, 1.2 parts by weight of mahogany petroleum sulfonate, 0.7 part by weight of mannan, 4.2 parts by weight of polypropylene oxide glycol and 0.4 part by weight of pomegranate bark powder sequentially and stirring continuously until the components are mixed completely and uniformly to prepare finishing liquid; 3) performing padding treatment on the fabric in the finishing liquid, taking out the fabric and drying the fabric at constant temperature. The fabric finished by the process has good properties and soft hand feeling.

Description

technical field [0001] The invention relates to a post-finishing process for brushed fabrics. Background technique [0002] The flame retardant, antistatic, mildew-proof, moth-proof, anti-bacterial, washable, shrink-proof, wrinkle-resistant and wear-resistant properties of the existing fabrics need to be improved, and the hand feeling is not soft enough. Contents of the invention [0003] The purpose of the present invention is to provide a finishing process for brushed fabrics, which has excellent flame retardant, antistatic, mildew-proof, moth-proof, antibacterial, washable, shrink-proof, wrinkle-resistant and wear-resistant properties. And feel soft. [0004] In order to achieve the above object, the technical solution of the present invention is to design a finishing process for brushed fabrics, comprising the steps of: [0005] 1) 1 to 2 parts by weight of alkyl dimethyl aryl ammonium chloride, 3.1 parts by weight of dithiocarbamic acid, 4.1 parts by weight of three...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): D06M13/463D06M13/425D06M13/224D06M15/09D06M15/03D06M15/53D06M15/01D06M13/256
CPCD06M13/224D06M13/256D06M13/425D06M13/463D06M15/01D06M15/03D06M15/09D06M15/53
Inventor 李启伟
Owner 常熟市鑫博伟针纺织有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products