A composite filter material and multi-functional technology, applied in separation methods, chemical instruments and methods, filtration and separation, etc., can solve problems such as aggravating farmland salinization, inability to clean sewage salinity, reducing crop production, etc., to ensure production , Good effect of purifying and removing peculiar smell
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0040] S1. Put 8 parts of rosin, 30 parts of polypropylene, 19 parts of zeolite powder and 23 parts of activated carbon in the mixing and stirring place for mixing and stirring, and stir for 10 minutes at a speed of 15 revolutions per second. After the stirring is completed, put the mixture into the double In a screw extruder and at a temperature of 270 degrees, the mixture is melted and extruded to form a first mixture.
[0041] S2. Put 8 parts of potassium chloride and 6 parts of sodium lauryl sulfate into 18 parts of water, then heat to 770 degrees, and stir for 5 minutes at a speed of 10 circles per second to completely dissolve , followed by adding 10 parts of potassium sulfate, and performing high-speed stirring at a speed of 10 revolutions per second for 3 minutes to obtain a second mixture.
[0042] S3. Put 10 parts of polytetrafluoroethylene into a high-speed grinder for grinding for ten minutes, grind it into powder, and put it aside for later use.
[0043] S4. Put ...
Embodiment 2
[0046] S1. Put 6 parts of rosin, 31 parts of polypropylene, 15 parts of zeolite powder and 15 parts of activated carbon in the mixing and stirring place for mixing and stirring, and stir for 10 minutes at a speed of 15 circles per second. After the stirring is completed, put the mixture into the double In a screw extruder and at a temperature of 270 degrees, the mixture is melted and extruded to form a first mixture.
[0047] S2. Put 7 parts of potassium chloride and 4 parts of sodium lauryl sulfate into 15 parts of water, then heat to 770 degrees, and stir for 5 minutes at a speed of 10 revolutions per second to completely dissolve , followed by adding 7 parts of potassium sulfate, and performing high-speed stirring at a speed of 10 revolutions per second for 3 minutes to obtain the second mixture.
[0048] S3. Put 8 parts of polytetrafluoroethylene into a high-speed grinder for grinding for ten minutes, grind it into powder, and put it aside for later use.
[0049] S4. Put ...
Embodiment 3
[0052] S1. Put 7 parts of rosin, 31 parts of polypropylene, 16 parts of zeolite powder and 16 parts of activated carbon in the mixing and stirring place for mixing and stirring, and stir for 10 minutes at a speed of 15 circles per second. After the stirring is completed, put the mixture into the double In a screw extruder and at a temperature of 270 degrees, the mixture is melted and extruded to form a first mixture.
[0053] S2. Put 9 parts of potassium chloride and 5 parts of sodium lauryl sulfate into 17 parts of water, then heat to 770 degrees, and stir for 5 minutes at a speed of 10 revolutions per second to completely dissolve , followed by adding 9 parts of potassium sulfate, and performing high-speed stirring at a speed of 10 revolutions per second for 3 minutes to obtain the second mixture.
[0054] S3. Put 11 parts of polytetrafluoroethylene into a high-speed grinder for grinding for ten minutes, grind it into powder, and put it aside for later use.
[0055]S4. Put ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com