[0016] A high-temperature water-soluble plastic film for medical use. The following weight components are weighed: 50 kg of polyvinyl alcohol, 8 kg of calcium carbonate, 1 kg of nano-titanium dioxide, 1 kg of nano-antimony trioxide, 7 kg of sodium alkylbenzenesulfonate, Tetrabutyl titanate 1.2kg, xylitol 12kg, starch phosphate 60kg, urea 2kg, magnesium stearate 1kg, acetyl tributyl citrate 13kg, citric acid 1kg, 3-hydroxybenzoic acid 4kg, polyvinylpyrrolidone 1kg, water-soluble wax flakes 4kg.
[0017] Made with the following specific steps:
[0018] (1) Mix phosphate starch and sodium alkylbenzene sulfonate evenly and put them in an oven, dry them at 130°C for 120 minutes, take them out, cool them to room temperature, and shake the mixed powder ultrasonically for 30-40 minutes (controlled The temperature of the water bath is 30°C, and the ultrasonic power is 100W), then the mixed powder is transferred to a stirring tank, and tetrabutyl titanate is added, the temperature is c...
Embodiment 2
[0023] A high-temperature water-soluble plastic film for medical use. The following components are weighed: 60 kg of polyvinyl alcohol, 15 kg of calcium carbonate, 4 kg of nano-titanium dioxide, 2 kg of nano-antimony trioxide, and 9 kg of sodium alkylbenzenesulfonate , Tetrabutyl titanate 1.4kg, Xylitol 14kg, Phosphate starch 65kg, Urea 3kg, Magnesium stearate 2kg, Acetyl tributyl citrate 15kg, Citric acid 1.5kg, 3-Hydroxybenzene Formic acid 6kg, polyvinylpyrrolidone 2kg, water-soluble wax flakes 6kg.
[0024] Made with the following specific steps:
[0025] (1) Mix phosphate starch and sodium alkylbenzene sulfonate evenly and put them in an oven, dry them at 130°C for 120 minutes, take them out, cool them to room temperature, and shake the mixed powder ultrasonically for 30-40 minutes (controlled The temperature of the water bath is 30°C, and the ultrasonic power is 100W), then the mixed powder is transferred to a stirring tank, and tetrabutyl titanate is added, the temperat...
Embodiment 3
[0030] A medical high-temperature water-soluble plastic film, the following components are weighed: 55 kg of polyvinyl alcohol, 10 kg of calcium carbonate, 3 kg of nano-titanium dioxide, 1.5 kg of nano-antimony trioxide, and 8 kg of sodium alkylbenzenesulfonate , Tetrabutyl titanate 1.3kg, Xylitol 13kg, Phosphate starch 63kg, Urea 2kg, Magnesium stearate 2kg, Acetyl tributyl citrate 13kg, Citric acid 1kg, 3-Hydroxybenzene Formic acid 5kg, polyvinylpyrrolidone 1kg, water-soluble wax flakes 5kg.
[0031] Made with the following specific steps:
[0032] (1) Mix phosphate starch and sodium alkylbenzene sulfonate evenly and put them in an oven, dry them at 130°C for 120 minutes, take them out, cool them to room temperature, and shake the mixed powder ultrasonically for 30-40 minutes (controlled The temperature of the water bath is 30°C, and the ultrasonic power is 100W), then the mixed powder is transferred to a stirring tank, and tetrabutyl titanate is added, the temperature is c...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com