Preparation method for low temperature resistant geogrid
A technology of geogrid and low temperature resistance, applied in the field of preparation of low temperature resistant geogrid, can solve problems such as inability to exert effect, and achieve the effect of improving chemical corrosion resistance, good compatibility and good dimensional stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A method for preparing a low-temperature resistant geogrid, comprising the following steps:
[0019] (1) Preparation of low-temperature resistance additive: by weight, 30 parts of alumina, 2 parts of 3-hydroxy-1-adamantaneacetic acid, 3 parts of N,N-dioctylglycine hydrochloride, 16 parts of titanium dioxide, two Put 14 parts of tungsten sulfide into a ball mill and mix at high speed for 60 minutes to obtain a low temperature resistant additive;
[0020] (2) In parts by weight, after mixing 90 parts of HDPE, 1 part of antioxidant DLTP, 4 parts of tetrabromobisphenol S, 1 part of heptamethylnonane, and 6 parts of dinonyl phthalate, put In the high-speed mixer, after high-speed mixing for 15 minutes, add the low-temperature resistant additive obtained in step (1) to it, and continue mixing for 11 minutes;
[0021] (3) putting the mixture obtained in step (2) into an extruder for melt extrusion to obtain a plate;
[0022] (4) Punch the plate obtained in step (3) through a...
Embodiment 2
[0028] A method for preparing a low-temperature resistant geogrid, comprising the following steps:
[0029] (1) Preparation of low-temperature resistant additives: in parts by weight, 35 parts of alumina, 3 parts of 3-hydroxy-1-adamantaneacetic acid, 5 parts of N,N-dioctylglycine hydrochloride, 18 parts of titanium dioxide, Put 16 parts of tungsten sulfide into a ball mill and mix at high speed for 70 minutes to obtain a low temperature resistant additive;
[0030] (2) In parts by weight, mix 93 parts of HDPE, 1 part of antioxidant DLTP, 5 parts of tetrabromobisphenol S, 2 parts of heptamethylnonane, and 7 parts of dinonyl phthalate. In the high-speed mixer, after high-speed mixing for 17 minutes, add the low-temperature resistance additive obtained in step (1) to it, and continue mixing for 13 minutes;
[0031] (3) putting the mixture obtained in step (2) into an extruder for melt extrusion to obtain a plate;
[0032] (4) Punch the plate obtained in step (3) through a punch...
Embodiment 3
[0038] A method for preparing a low-temperature resistant geogrid, comprising the following steps:
[0039] (1) Preparation of low-temperature resistant additives: by weight, 40 parts of alumina, 4 parts of 3-hydroxy-1-adamantaneacetic acid, 6 parts of N,N-dioctylglycine hydrochloride, 19 parts of titanium dioxide, two Put 17 parts of tungsten sulfide into a ball mill and mix at high speed for 80 minutes to obtain a low temperature resistant additive;
[0040] (2) In parts by weight, mix 95 parts of HDPE, 2 parts of antioxidant DLTP, 6 parts of tetrabromobisphenol S, 3 parts of heptamethylnonane, and 8 parts of dinonyl phthalate. In the high-speed mixer, after high-speed mixing for 20 minutes, add the low-temperature resistant additive obtained in step (1) to it, and continue mixing for 15 minutes;
[0041] (3) putting the mixture obtained in step (2) into an extruder for melt extrusion to obtain a plate;
[0042] (4) Punch the plate obtained in step (3) through a punching m...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com