Low-wear environment-friendly shield tail sealing grease and preparation method thereof
An environment-friendly, shield tail sealing technology, applied in the petroleum industry, lubricating compositions, etc., can solve the problems of uneven varieties, high wear, unfavorable performance optimization, etc., and achieve the effect of good pumpability and low wear
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0016] A shield tail sealing grease, its components and mass percentages are as follows:
[0017] 25% soybean oil, 23% mica powder, 8.9% sepiolite fiber, 5.3% graphene, 17.8% castor oil, 6% rosin, 3% acetone, etc., 2% octadecylamine polyoxyethylene ether, 9 polyacryl alcohol %.
[0018] The preparation method is as follows: 25% soybean oil, 8.9% sepiolite fiber, 5.3% graphene, and 17.8% castor oil are mixed into a reaction kettle, and heated to above 100°C until the mixture is uniform. Add 3% acetone to the mixture, and stir at constant temperature until the mixture is uniform. Then add 6% rosin, 9% polypropylene alcohol, and 2% octadecylamine polyoxyethylene ether to raise the temperature to 140°C, then add 23% mica powder, keep warm and continue stirring at low speed for 2 to 3 hours.
Embodiment 2
[0020] A shield tail sealing grease, its components and mass percentages are as follows:
[0021] 22% peanut oil, 13% dioctyl terephthalate, 24% bentonite, 24% asbestos fiber, 6% polyacrylamide, 7% coumarone resin, 2% propylene carbonate, 2 stearylamine polyoxyethylene ether %.
[0022] The preparation method is as follows: mix 22% of peanut oil, 13% of dioctyl terephthalate, and 24% of asbestos fiber into a reaction kettle, and heat to above 100°C until the mixture is uniform. Add polyacrylamide 6% into the mixture, and stir at constant temperature until the mixture is uniform. Then add coumarone resin, 2% propylene carbonate, and 2% octadecylamine polyoxyethylene ether to raise the temperature to 140°C, then add 24% bentonite, keep warm and continue stirring at low speed for 2 to 3 hours.
[0023] The product quality of the embodiment of the present invention 1 and embodiment 2 is as follows:
[0024]
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com