Preparation method of finished hemp and bamboo toilet paper product
A technology of toilet paper and hemp bamboo, applied in the direction of textile and paper making, paper making, paper machine, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0038] In an embodiment, the preparation method of the finished hemp bamboo toilet paper includes the following steps:
[0039] S1: Cut the hemp bamboo into slices of 20-30×2.8-3.7mm×1.2-2.5mm in size and pulverize, and the obtained pulverized material is transported to the primary pretreatment infusion A. The weight of the pulverized material The ratio to the volume of the primary pretreatment immersion liquid A is 1:1.5-3.5. The primary pretreatment immersion liquid A is in parts by weight and includes the following raw materials: 4-8 parts of alkylphenol polyoxyethylene ether and 0.3 of triethanolamine -0.6 parts, stearic acid 0.5-1 parts, oleic acid 0.4-1.2 parts, lauric acid 0.8-1.5 parts, water 42-90 parts, soaked at an ultrasonic power of 30-50W and a temperature of 43-48℃26 -40min, then filter to obtain leaching material A;
[0040] S2: Transport the leaching material A prepared in step S1 to the secondary pretreatment immersion liquid B, the ratio of the weight of the lea...
Embodiment 1
[0048] A preparation method of finished hemp bamboo toilet paper includes the following steps:
[0049] S1: Cut the hemp bamboo into slices of hemp bamboo with a size of 22×3.2mm×1.3mm and pulverize, and the obtained pulverized material is transported to the primary pretreatment immersion liquid A, and the weight of the sesame bamboo pulverized material and the primary pretreatment immersion liquid The volume ratio of A is 1:1.6. The primary pretreatment leaching solution A is in parts by weight and includes the following raw materials: 4 parts of alkylphenol polyoxyethylene ether, 0.3 parts of triethanolamine, 0.5 parts of stearic acid, and oleic acid 0.4 parts, 0.8 parts of lauric acid, 42 parts of water, immersed in ultrasonic power of 30W and temperature of 43℃ for 40min, and then filtered to obtain leaching material A;
[0050] S2: The leaching material A prepared in step S1 is transported to the secondary pretreatment immersion liquid B, the ratio of the weight of the leachin...
Embodiment 2
[0058] A preparation method of finished hemp bamboo toilet paper includes the following steps:
[0059] S1: Cut the hemp bamboo into pieces of hemp bamboo with a size of 29×3.6mm×2.4mm and pulverize, and the obtained pulverized material is transported to the primary pretreatment immersion solution A, and the weight of the sesame bamboo pulverized material is compared with the primary pretreatment immersion solution The volume ratio of A is 1:3.4. The primary pretreatment leaching solution A is based on parts by weight and includes the following raw materials: 8 parts of alkylphenol polyoxyethylene ether, 0.6 parts of triethanolamine, 1 part of stearic acid, and oleic acid -1.2 parts, 1.5 parts of lauric acid, 90 parts of water, immersed in an ultrasonic power of 50W and a temperature of 48°C for 26min, and then filtered to obtain leaching material A;
[0060] S2: Transport the leaching material A obtained in step S1 to the secondary pretreatment immersion liquid B, the ratio of the...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com