Preparation method of novel energy-saving flame-retardant building material
A building material and a new type of technology, applied in the field of building materials, can solve the problems of high addition amount, unsatisfactory heat insulation effect, and no crack resistance, and achieve the effects of good flame retardancy, improved fusion performance and low cost.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A method for preparing a novel energy-saving and flame-retardant building material, comprising the following steps:
[0026] 1. Grinding magnesium oxide into 2000 mesh, mixing it with magnesium sulfate and building material additives, and then crushing it into 3500 mesh to obtain mixture 1;
[0027] 2. Take silicon dioxide powder and nano-silicon carbide powder by mass ratio, and use dehydrated alcohol as a dispersion medium for the silicon dioxide and silicon carbide powder that has been weighed, and obtain mixture 2 after dispersion;
[0028] 3. Put mixture 2 into a nylon ball mill jar, use agate balls as grinding balls, and obtain mixture 3 after ball milling;
[0029] 4. Pour the mixture 3 together with the agate balls into the powder tray, dry and sieve at 100°C, take out the agate balls, and grind to obtain the mixture 4;
[0030] 5. Mix mixture 1 and mixture 4 with graphene evenly, and press to form.
[0031] The new energy-saving and flame-retardant building m...
Embodiment 2
[0039] A method for preparing a novel energy-saving and flame-retardant building material, comprising the following steps:
[0040] 1. Grinding magnesium oxide into 2000 mesh, mixing it with magnesium sulfate and building material additives, and then crushing it into 4200 mesh to obtain mixture 1;
[0041] 2. Take silicon dioxide powder and nano-silicon carbide powder by mass ratio, and use dehydrated alcohol as a dispersion medium for the silicon dioxide and silicon carbide powder that has been weighed, and obtain mixture 2 after dispersion;
[0042] 3. Put mixture 2 into a nylon ball mill jar, use agate balls as grinding balls, and obtain mixture 3 after ball milling;
[0043] 4. Pour the mixture 3 together with the agate balls into the powder tray, dry and sieve at 150°C, take out the agate balls, and grind to obtain the mixture 4;
[0044] 5. Mix mixture 1 and mixture 4 with graphene evenly, and press to form.
[0045] The new energy-saving flame-retardant building mater...