A technology of mechanical equipment and lubricating oil, which is applied in the direction of lubricating composition and petroleum industry, etc. It can solve the problems of large friction power consumption and wear of equipment, large environmental pollution of lubricating oil, and large consumption of lubricating oil, so as to reduce the energy consumption of operation , reduce the friction coefficient, reduce the effect of consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A preparation method for lubricating oil for mechanical equipment, comprising the following preparation methods:
[0026] a. Mix the modified nano-copper powder, detergent, dispersant, preservative, extreme pressure anti-wear agent and oily agent and stir at high speed for 50 minutes at a stirring speed of 600r / min to obtain mixture 1;
[0027] b. Mix antioxidant, viscosity index improver, rust inhibitor, pour point depressant, antifoaming agent and base oil evenly in a reaction kettle, knead at 180°C for 20 minutes, cool to room temperature, and obtain mixture 2 ;
[0028] c. Mix mixture 1 and mixture 2, heat at 100°C, and concentrate to obtain the finished product.
[0029] The lubricating oil includes the following raw materials in parts by weight: 23 parts of modified nano-copper powder, 6 parts of detergent, 3 parts of dispersant, 4 parts of preservative, 7 parts of extreme pressure antiwear agent, 7 parts of oiliness agent, and 6 parts of antioxidant , 5 parts o...
Embodiment 2
[0037] A preparation method for lubricating oil for mechanical equipment, comprising the following preparation methods:
[0038] a. Mix the modified nano-copper powder, detergent, dispersant, preservative, extreme pressure anti-wear agent and oily agent and stir at a high speed for 30 minutes at a stirring speed of 800r / min to obtain a mixture 1;
[0039] b. Mix the antioxidant, viscosity index improver, rust inhibitor, pour point depressant, antifoaming agent and base oil evenly in the reactor, knead at 180°C for 30 minutes, cool to room temperature, and obtain the mixture II ;
[0040] c. Mix mixture 1 and mixture 2, heat at 100°C, and concentrate to obtain the finished product.
[0041] The lubricating oil includes the following raw materials in parts by weight: 28 parts of modified nano-copper powder, 6 parts of detergent, 7 parts of dispersant, 4 parts of preservative, 7 parts of extreme pressure antiwear agent, 7 parts of oiliness agent, and 8 parts of antioxidant , 8 pa...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com