Antistatic breathable down used for down jackets and a preparing method thereof
An anti-static, down jacket technology, applied in the field of clothing fabrics, can solve the problems of bloated products, soaring down costs, high prices, etc., achieve good anti-static and breathability, improve beauty and comfort, and stability. The effect of little change
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] A preparation method of antistatic and breathable down for down wear, the specific steps are:
[0014] Cross-linking modification treatment: throw the down into a solution with a cyclodextrin concentration of 12.8g / L, a citric acid concentration of 3.5g / L, a sodium hypophosphite concentration of 2.4g / L, and an active polypeptide concentration of 0.0022g / L. React for 4.5 hours at a bath ratio of 1:150 and a temperature of 80°C. After the reaction is completed, wash with clean water three times and dry in an oven at 80°C to obtain modified down. The amino acid sequence of the active peptide is HSHACKCGAAKCYLCRVLHPGKLCVCNCSK This active peptide can destroy the lipids composed of the cell membrane of the bimolecular layer of alcohol and triphosphate on the down surface, reduce the surface tension of the solution, make the down easier to disperse in water, and increase the contact between the small cyclodextrin molecules and the down. Step: The cyclodextrin is grafted to the su...
Embodiment 2
[0018] A preparation method of antistatic and breathable down for down wear, the specific steps are:
[0019] 1) Put down into a solution with a cyclodextrin concentration of 14g / L, a citric acid concentration of 3g / L, a sodium hypophosphite concentration of 2.1g / L, and an active peptide concentration of 0.0025g / L, at a bath ratio of 1: 140. React at 75℃ for 5 hours, wash and dry, and then get modified down. The amino acid sequence of the active peptide is HSHACKCGAAKCYLCRVLHPGKLCVCNCSK. This active peptide can destroy the lipids composed of the cell membrane of the bimolecular layer of alcohol and triphosphate on the surface of down , Reduce the surface tension of the solution, make the down easier to disperse in the water, increase the contact between the small cyclodextrin molecules and the down, this step grafts the cyclodextrin to the down surface through the small molecules, which can increase the hydrophilicity of the down. The reaction of down in an aqueous solution is ea...
Embodiment 3
[0023] A preparation method of antistatic breathable down for down taking, the specific steps are: putting down into cyclodextrin concentration of 12.5g / L, citric acid concentration of 3.7g / L, sodium hypophosphite concentration of 2g / L, active polypeptide concentration In a solution of 0.003g / L, react for 4h at a bath ratio of 1:145 and a temperature of 80℃, wash and dry; put the modified down into a 22g / L methylammonium methyl sulfate salt Soak in the solution for 2 minutes, take it out, and pre-bake at 96°C for 2.5 minutes, and then bake it at 170°C for 110 seconds; put the antistatic treated down into a hydrogen peroxide solution with a concentration of 36mL / L, and adjust the pH to 5, Treat for 30min at ℃, cool down, wash with water to neutral, dry, and set aside.
[0024] The conventional operations in the operation steps of the present invention are well known to those skilled in the art, and will not be repeated here.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com