A kind of natural degradable macromolecule haze suppressing spray agent and its preparation method and application
A technology of macromolecules and spraying agents, which is applied in the field of air pollution control and can solve problems such as products that do not solve the hazards of smog
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] Preparation of natural degradable macromolecule haze suppression spraying agent:
[0030] 1) Weigh 10 g of acrylic acid, slowly add 4 g of the cooled sodium hydroxide solution prepared in Embodiment 1 under ice bath conditions, and keep stirring. solution;
[0031] 2) 1g of humic acid solution prepared in Embodiment 1, 2g of lignin solution, 0.2g of potassium persulfate solution, 0.03g of nitrogen nitrogen methylene bisacrylamide solution, 0.05g of nano-silver solution, and step 1) Add the reaction solution into the flask and stir evenly, adjust the pH value of the reaction system to 2, stir vigorously with an electric stirrer at 400r / min for 2 hours, put it in a microwave oven at 300W to initiate the reaction and react for 10min, take it out, filter it with suction, and wash it with ethanol for 2 hours Then, vacuum-dried at 30°C for 48 hours, and pulverized to obtain the natural degradable macromolecular haze suppression spray agent, wherein the pulverized particle si...
Embodiment 2
[0033] Preparation of natural degradable macromolecule haze suppression spraying agent:
[0034] 1) Weigh 12 g of acrylic acid, slowly add 4 g of the cooled sodium hydroxide solution prepared in Embodiment 1 under ice bath conditions, and keep stirring, after the neutralization is completed, place the solution temperature in the ice bath to room temperature to obtain a reaction solution ;
[0035] 2) 0.7g of humic acid solution prepared in Embodiment 1, 4g of lignin solution, 0.3g of potassium persulfate solution, 0.06g of nitrogen nitrogen methylenebisacrylamide solution, 0.08g of nano-silver solution, and step 1) The reaction solution was added to the flask and stirred evenly, then the pH value of the reaction system was adjusted to 3, stirred vigorously with an electric stirrer at 500r / min for 1.5 hours, put into a microwave oven at 500W to initiate the reaction and reacted for 5min, then took it out, and washed it with ethanol for 3 and then vacuum-dried at 35° C. for 40 ...
Embodiment 3
[0037] Preparation of natural degradable macromolecule haze suppression spraying agent:
[0038] 1) Weigh 8 g of acrylic acid, slowly add 4.3 g of the cooled sodium hydroxide solution prepared in Embodiment 1 under ice bath conditions, and keep stirring, and after neutralization, place it in an ice bath until the solution temperature reaches room temperature to obtain reaction solution;
[0039] 2) 1.5g of humic acid solution prepared in Embodiment 1, 7g of lignin solution, 0.4g of potassium persulfate solution, 0.07g of nitrogen nitrogen methylenebisacrylamide solution, 0.03g of nano silver solution, and step 1) Add the reaction solution into the flask and stir evenly, adjust the pH value of the reaction system to 2.5, stir vigorously with an electric stirrer at 800r / min for 1 hour, put it in a microwave oven at 300W to initiate the reaction and react for 25min, take it out, and wash it with ethanol by suction filtration , followed by vacuum drying at 30° C. for 45 hours, an...
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle diameter | aaaaa | aaaaa |
| particle diameter | aaaaa | aaaaa |