Building material with high toughness and good water resistance and having anti-cracking effect and preparation method of building material
A technology of building materials and water resistance, which is applied in the field of building materials with high toughness, good water resistance and crack resistance and its preparation. It can solve problems such as poor toughness, water leakage in the house, and general effect, and achieve the probability of cracking and breaking. Reduce and improve the ability to resist deformation and change the effect of mechanical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Building materials with high toughness, good water resistance and crack resistance, including the following raw materials in proportion by weight: 20 parts of composite fiber material, 30 parts of Portland cement, 10 parts of calcium carbonate, 5 parts of fly ash, silica fume 3 parts, 1 part of copper stearate, 0.5 parts of polycarboxylate, 1 part of methyl cellulose, 1 part of ethylene-vinyl acetate copolymer, 10 parts of polyurethane, 10 parts of water-based bitumen base, 8 parts of polyvinyl chloride and 7 parts of soap emulsified asphalt.
[0024] A preparation method for a building material with high toughness, good water resistance and crack resistance, comprising the following steps:
[0025] 1) Pour 20 parts of composite fiber material, 30 parts of Portland cement, 10 parts of calcium carbonate, 5 parts of fly ash and 3 parts of silicon powder into the mixer and stir at a speed of 100RPS for 1 hour. Standby:
[0026] 2) Pour 1 part of copper stearate, 0.5 part ...
Embodiment 2
[0030] Building materials with high toughness, good water resistance and crack resistance, including the following raw materials in proportion by weight: 30 parts of composite fiber material, 40 parts of Portland cement, 12 parts of calcium carbonate, 7 parts of fly ash, silica fume 5 parts, copper stearate 2.5 parts, polycarboxylate 1.5 parts, methyl cellulose 2 parts, ethylene-vinyl acetate copolymer 1.5 parts, polyurethane 11 parts, water-based bitumen base 14 parts, polyvinyl chloride 9 parts and Soap emulsified asphalt 8 parts.
[0031] A method for preparing a building material with high toughness, good water resistance and crack resistance, comprising the following steps:
[0032] 1) Pour 30 parts of composite fiber material, 40 parts of Portland cement, 12 parts of calcium carbonate, 7 parts of fly ash and 5 parts of silicon powder into the mixer and stir at a speed of 150RPS for 1.5 hours. Standby:
[0033] 2) Pour 2.5 parts of copper stearate, 1.5 parts of polycarbo...
Embodiment 3
[0037] Building materials with high toughness, good water resistance and crack resistance, including the following raw materials in proportion by weight: 40 parts of composite fiber material, 50 parts of Portland cement, 15 parts of calcium carbonate, 10 parts of fly ash, silica fume 7 parts, copper stearate 4 parts, polycarboxylate 2 parts, methyl cellulose 3 parts, ethylene-vinyl acetate copolymer 2 parts, polyurethane 12 parts, water-based bitumen base 18 parts, polyvinyl chloride 10 parts and 9 parts of soap emulsified asphalt.
[0038] A method for preparing a building material with high toughness, good water resistance and crack resistance, comprising the following steps:
[0039] 1) Pour 40 parts of composite fiber material, 50 parts of Portland cement, 15 parts of calcium carbonate, 10 parts of fly ash and 7 parts of silicon powder into the mixer and stir at a speed of 200RPS for 2 hours. Standby:
[0040]2) Pour 4 parts of copper stearate, 2 parts of polycarboxylate,...