Jewelry 10K black gold with excellent abrasion resisting performance and technology of jewelry 10K black gold
A wear-resistant, 10K technology, applied in the field of gold alloys, can solve the problems of difficult processing, weak core competitiveness, and small scale of enterprises, and achieve stable corrosion resistance, excellent cold and hot processing performance, and excellent friction resistance. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A kind of 10K black gold with excellent wear resistance for jewelry and its technology. In terms of weight percentage, the composition of the alloy is Sr: 0.5wt.%, Zn: 2.0wt.%, Ca: 1.0wt.%, Nb: 1.4wt.%, Sn: 18.0wt.%, Fe: 10.0wt.% , Au: 40.0wt.%, the balance is cobalt. The above-mentioned 10K black gold with excellent wear resistance and its technology for jewelry use include the following steps: adding the raw materials in the above ratio into an argon-protected induction furnace, and using a graphite crucible; Protected by argon gas to avoid serious burning of alloy elements due to large air flow; heat preservation at 1200 degrees for 10 minutes during smelting, and electromagnetic stirring by high-frequency induction furnace; after stirring evenly, heat preservation at 1200 degrees for 1 minute and cast out of the furnace; gold alloy casting adopts The steel mold with a diameter of 50-100mm is cooled by water cooling. The obtained ingot is rolled at room temperature...
Embodiment 2
[0020]A kind of 10K black gold with excellent wear resistance for jewelry and its technology. In terms of weight percentage, the composition of the alloy is Sr: 0.8wt.%, Zn: 3.5wt.%, Ca: 1.5wt.%, Nb: 1.8wt.%, Sn: 20.0wt.%, Fe: 15.0wt.% , Au: 42.0wt.%, the balance is cobalt. The above-mentioned 10K black gold with excellent wear resistance and its technology for jewelry use include the following steps: adding the raw materials in the above ratio into an argon-protected induction furnace, and using a graphite crucible; Protected by argon gas to avoid serious burning of alloy elements due to large air flow; heat preservation at 1200 degrees for 10 minutes during smelting, and electromagnetic stirring by high-frequency induction furnace; after stirring evenly, heat preservation at 1200 degrees for 1 minute and cast out of the furnace; gold alloy casting adopts The steel mold with a diameter of 50-100mm is cooled by water cooling. The obtained ingot is rolled at room temperature,...
Embodiment 3
[0023] A kind of 10K black gold with excellent wear resistance for jewelry and its technology. In terms of weight percentage, the composition of the alloy is Sr: 0.6wt.%, Zn: 2.4wt.%, Ca: 1.2wt.%, Nb: 1.5wt.%, Sn: 16.0wt.%, Fe: 12.0wt.% , Au: 41.0wt.%, the balance is cobalt. The above-mentioned 10K black gold with excellent wear resistance and its technology for jewelry use include the following steps: adding the raw materials in the above ratio into an argon-protected induction furnace, and using a graphite crucible; Protected by argon gas to avoid serious burning of alloy elements due to large air flow; heat preservation at 1200 degrees for 10 minutes during smelting, and electromagnetic stirring by high-frequency induction furnace; after stirring evenly, heat preservation at 1200 degrees for 1 minute and cast out of the furnace; gold alloy casting adopts The steel mold with a diameter of 50-100mm is cooled by water cooling. The obtained ingot is rolled at room temperature...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com