Efficient flame-retardant wear-resistant subway cable and preparation method thereof
A subway and high-efficiency technology, applied in the direction of rubber insulators, organic insulators, etc., can solve the problems of troublesome staff, complicated maintenance and replacement work, poor flame retardancy and wear resistance, etc., to achieve performance synergy, reduce temperature, improve Effect of Tensile Strength and Elongation at Break
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] A high-efficiency flame-retardant and wear-resistant subway cable, comprising the following raw materials in proportions by weight: 20 parts of silicone rubber, 5 parts of EPDM rubber, 3 parts of butyl rubber, 3 parts of polyurethane, and acetyl trioctyl citrate 3 parts, 10 parts of modified alumina, 10 parts of kaolin, 10 parts of microencapsulated red phosphorus, 5 parts of zinc borate, 2 parts of 3-aminopropyltriethoxysilane, 1 part of accelerator, Ca / Zn compound stabilizer 2 parts of anti-aging agent, 1 part of anti-aging agent, 3 parts of silicone powder and cables.
[0028] Further, the cable includes a metal core and an insulating layer.
[0029] Further, the modifier of modified alumina is one of hexadecyltrimethoxysilane, γ-aminopropyltriethoxysilane, and vinyltris(β-methoxyethoxy)silane or a variety of combinations.
[0030] Further, the antioxidant is one or more of N-phenyl-α-aniline, N-phenyl-β-naphthylamine, p-phenylenediamine and N-N'-diphenyl-p-phenyle...
Embodiment 2
[0040] A high-efficiency flame-retardant and wear-resistant subway cable, comprising the following raw materials in proportions by weight: 30 parts of silicone rubber, 10 parts of EPDM rubber, 5.5 parts of butyl rubber, 6.5 parts of polyurethane, and acetyl trioctyl citrate 3.5 parts, 15 parts of modified alumina, 12.5 parts of kaolin, 12.5 parts of microencapsulated red phosphorus, 7.5 parts of zinc borate, 4 parts of 3-aminopropyltriethoxysilane, 1.5 parts of accelerator, Ca / Zn composite stability 3 parts of anti-aging agent, 2 parts of anti-aging agent, 5 parts of silicone powder and cables.
[0041] Further, the cable includes a metal core and an insulating layer.
[0042] Further, the modifier of modified alumina is one of hexadecyltrimethoxysilane, γ-aminopropyltriethoxysilane, and vinyltris(β-methoxyethoxy)silane or a variety of combinations.
[0043] Further, the antioxidant is one or more of N-phenyl-α-aniline, N-phenyl-β-naphthylamine, p-phenylenediamine and N-N'-d...
Embodiment 3
[0053] A high-efficiency flame-retardant and wear-resistant subway cable, comprising the following raw materials in proportions by weight: 40 parts of silicone rubber, 15 parts of EPDM rubber, 8 parts of butyl rubber, 10 parts of polyurethane, and acetyl trioctyl citrate 4 parts, 20 parts of modified alumina, 115 parts of kaolin, 15 parts of microencapsulated red phosphorus, 10 parts of zinc borate, 6 parts of 3-aminopropyltriethoxysilane, 2 parts of accelerator, Ca / Zn compound stabilizer 4 parts of anti-aging agent, 3 parts of anti-aging agent, 7 parts of silicone powder and cables.
[0054] Further, the cable includes a metal core and an insulating layer.
[0055] Further, the modifier of modified alumina is one of hexadecyltrimethoxysilane, γ-aminopropyltriethoxysilane, and vinyltris(β-methoxyethoxy)silane or a variety of combinations.
[0056] Further, the antioxidant is one or more of N-phenyl-α-aniline, N-phenyl-β-naphthylamine, p-phenylenediamine and N-N'-diphenyl-p-p...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com