Remediation agent applicable to heavy metal pollution of southern acid rice field soil and preparation method of remediation agent
A remediation agent and heavy metal technology, applied in the field of soil pollution control, can solve problems such as poor targeting, achieve light targeting, ensure remediation effect and efficiency, and reduce cadmium well.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] A remediation agent suitable for heavy metal pollution in southern acid paddy soil, comprising 12 parts by weight of chelated manganese, 1.5 parts of silicon dioxide, 28 parts of zinc sulfate, 1.7 parts of magnesium phosphate, 0.8 parts of ferrous sulfate, and 1.2 parts of sulfur 1 part, 1 part of calcium oxide and 120 parts of bentonite.
[0027] Chelated Manganese as EDTA•Na 2 Mn;
[0028] Bentonite is (Na,Ca)0.33(Al,Mg) 2 [Si 4 O10](OH) 2 •nH 2 O.
[0029] Its preparation method comprises the following steps:
[0030] A Immerse bentonite of a certain fineness (120-200 mesh) in sulfuric acid, hydrochloric acid or phosphoric acid solution, mix well, wash with distilled water until nearly neutral, and after suction filtration, dry the solid at 110°C for 1.5-2 hours to obtain acid-activated bentonite . Add the acidified bentonite to a highly dispersed mercapto reagent in a water-soluble solvent, the ratio of acidic bentonite to mercapto reagent is 1:1.5, stir and...
Embodiment 2
[0036] A remediation agent suitable for heavy metal pollution in southern acid paddy soil, comprising 8 parts of chelated manganese, 2 parts of silicon dioxide, 25 parts of zinc sulfate, 3 parts of magnesium phosphate, 0.8 parts of ferrous sulfate, and 1 part of sulfur in parts by weight parts, 0.8 parts of calcium oxide and 120 parts of bentonite.
[0037] Chelated Manganese as EDTA•Na 2 Mn;
[0038]Bentonite is (Na,Ca)0.33(Al,Mg) 2 [Si 4 o 10 ](OH) 2 •nH 2 O.
[0039] Its preparation method comprises the following steps:
[0040] A Immerse bentonite of a certain fineness (120-200 mesh) in sulfuric acid, hydrochloric acid or phosphoric acid solution, mix well, wash with distilled water until nearly neutral, and after suction filtration, dry the solid at 110°C for 1.5-2 hours to obtain acid-activated bentonite . Add the acidified bentonite to a highly dispersed mercapto reagent in a water-soluble solvent, the ratio of acidic bentonite to mercapto reagent is 1:1.5, sti...
Embodiment 3
[0046] A remediation agent suitable for heavy metal pollution in southern acid paddy soil, comprising 16 parts by weight of chelated manganese, 0.5 parts of silicon dioxide, 30 parts of zinc sulfate, 1 part of magnesium phosphate, 0.8 parts of ferrous sulfate, and 1.5 parts of sulfur Parts, 1.2 parts of calcium oxide and 120 parts of bentonite.
[0047] Chelated Manganese as EDTA•Na 2 Mn;
[0048] Bentonite is (Na,Ca)0.33(Al,Mg)2[Si4O10](OH)2•nH2O.
[0049] Its preparation method comprises the following steps:
[0050] A Immerse bentonite of a certain fineness (120-200 mesh) in sulfuric acid, hydrochloric acid or phosphoric acid solution, mix well, wash with distilled water until nearly neutral, and after suction filtration, dry the solid at 110°C for 1.5-2 hours to obtain acid-activated bentonite . Add the acidified bentonite to a highly dispersed mercapto reagent in a water-soluble solvent, the ratio of acidic bentonite to mercapto reagent is 1:1.5, stir and react at roo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com