Application of expanded glass beads in sand-in-water base paint, sand-in-water base paint, preparation method and sand-in-water coating
A technology of expanded vitrified microbeads and basic paint, which is applied in the field of imitation stone materials, can solve the problems of inability to achieve colorful visual effects of imitation marble, difficult particle shearing evenly, large proportion of sand particles in water, etc., so as to improve the suspension. , uniform size, stable physical and chemical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0037] A kind of sand-in-water base paint, it obtains by following processing steps:
[0038]Add 20 kg of deionized water into the mixing tank, start the mixer, and add 200 g of dispersant, 200 g of defoamer, 1 kg of antifreeze, 1 kg of film-forming aid, 1 kg of expanded vitrified microbeads, titanium 1kg of white powder, 1kg of kaolin and 0.8kg of hydroxyethyl cellulose were stirred and dispersed for 8 minutes; 1kg of multifunctional amine was added, and mixed at a high speed of 1500r / min for 15 minutes to obtain mixture A;
[0039] Add 20kg of emulsion, 100g of preservative, 5kg of 10wt% protective colloid solution, 500g of thickener and 40kg of quartz sand to Mixture A in sequence, and stir to disperse at 1000r / min 8 minutes to get the sand-in-water base paint.
Embodiment 2
[0041] A kind of sand-in-water base paint, it obtains by following processing steps:
[0042] Add 20kg of deionized water into the mixing tank, start the mixer, and add 200g of dispersant, 200g of defoamer, 1kg of antifreeze, 1kg of film-forming aid, 1kg of expanded vitrified microbeads, titanium 1kg of white powder, 1kg of kaolin and 0.8kg of hydroxyethyl cellulose were stirred and dispersed for 5 minutes; 1kg of multifunctional amine was added, and at a speed of 1300r / min, high-speed stirring was dispersed for 20 minutes to obtain mixture A;
[0043] Add 20kg of emulsion, 100g of preservative, 5kg of 10wt% protective colloid solution, 500g of thickener and 40kg of quartz sand to Mixture A in sequence, and stir to disperse at 900r / min After 10 minutes, the sand-in-water base paint was obtained.
Embodiment 3
[0045] A kind of sand-in-water base paint, it obtains by following processing steps:
[0046] Add 20kg of deionized water into the mixing tank, start the mixer, and add 200g of dispersant, 200g of defoamer, 1kg of antifreeze, 1kg of film-forming aid, 1kg of expanded vitrified microbeads, titanium 1kg of white powder, 1kg of kaolin and 0.8kg of hydroxyethyl cellulose were stirred and dispersed for 3 minutes; 1kg of multifunctional amine was added, and mixed at a high speed of 1200r / min for 25 minutes to obtain mixture A;
[0047] Add 20kg of emulsion, 100g of preservative, 5kg of 10wt% protective colloid solution, 500g of thickener and 40kg of quartz sand in sequence to Mixture A at a speed of 800r / min, and stir to disperse After 13 minutes, the sand-in-water base paint was obtained.
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com