The technology of capsaicin and antifouling agent is applied in the field of marine antifouling paint and underwater paint, which can solve the problems of endangering human health and safety, increasing fuel consumption, increasing ship maintenance costs, etc., and improving mechanical properties and anti-settling properties. , Prevent sustained release, reduce the effect of antifouling effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] Add 1 part of synthetic capsaicin into a four-neck flask, add 200mL of sterilized deionized water, make the liquid surface submerge the stirring paddle, place the four-necked flask on a constant temperature water bath for heating and stirring, and set the initial temperature of the constant temperature water bath The temperature is 85°C, and the stirring rod speed is set to 300r / min. After half an hour, the stirring paddle speed is reduced, and 2 parts of diatomite are weighed and slowly added to the four-necked flask, and the speed is increased to 450r / min to make the diatomite evenly Disperse in the capsaicin suspension, remove the water bath after 10 minutes, reduce the speed to 300r / min, and at the same time pass cooling water to the surface of the four-necked flask until the liquid in the four-necked flask drops to room temperature, so that the capsaicin crystals are precipitated and deposited On the diatomite, reduce the speed after 30 minutes, add acrylic acid sel...
Embodiment 2
[0028] Add 1 part of synthetic capsaicin into a four-neck flask, add 200mL of sterilized deionized water, make the liquid surface submerge the stirring paddle, place the four-necked flask on a constant temperature water bath for heating and stirring, and set the initial temperature of the constant temperature water bath The temperature is 85°C, and the stirring rod speed is set to 300r / min. After half an hour, the stirring paddle speed is reduced, and 2 parts of diatomite are weighed and slowly added to the four-necked flask, and the speed is increased to 450r / min to make the diatomite evenly Disperse in the capsaicin suspension, remove the water bath after 10 minutes, reduce the speed to 300r / min, and at the same time pass cooling water to the surface of the four-necked flask until the liquid in the four-necked flask drops to room temperature, so that the capsaicin crystals are precipitated and deposited On the diatomite, reduce the speed after 30 minutes, add acrylic acid sel...
Embodiment 3
[0030]Add 1 part of synthetic capsaicin into a four-neck flask, add 200mL of sterilized deionized water, make the liquid surface submerge the stirring paddle, place the four-necked flask on a constant temperature water bath for heating and stirring, and set the initial temperature of the constant temperature water bath The temperature is 85°C, and the stirring rod speed is set to 300r / min. After half an hour, the stirring paddle speed is reduced, and 2 parts of diatomite are weighed and slowly added to the four-necked flask, and the speed is increased to 450r / min to make the diatomite evenly Disperse in the capsaicin suspension, remove the water bath after 10 minutes, reduce the speed to 300r / min, and at the same time pass cooling water to the surface of the four-necked flask until the liquid in the four-necked flask drops to room temperature, so that the capsaicin crystals are precipitated and deposited On the diatomite, reduce the speed after 30 minutes, add acrylic acid self...