Deodorizing dressing with high comfort and air permeability and preparation method thereof
A breathable and comfortable technology, applied in the field of medical dressings, can solve the problems of patient discomfort and pain, long wound healing time, and low comfort, so as to reduce burden and distress, reduce the possibility of secondary infection, and improve permeability Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] (1) 890g vaseline and 89g liquid paraffin are mixed evenly, and set aside;
[0027] (2) Take 100g of the above-mentioned mixed solution obtained in step (1), add 1g of bismuth tribromophenate to it, and mix well;
[0028] (3) Add 10g of α-cyclodextrin to the mixed solution in the above step (2) to obtain a mixed slurry;
[0029] (4) Add the mixed slurry obtained in step (3) into the coating machine, dip the gauze overcoating slurry, apply 150 grams of slurry per square meter of gauze, and fold it after coating to obtain a hemostatic and detoxifying solution. Smelly dressing.
Embodiment 2
[0031] (1) 890g vaseline and 89g liquid paraffin are mixed evenly, and set aside;
[0032] (2) Take 100g of the above-mentioned mixed solution obtained in step (1), add 1g of bismuth tribromophenate to it, and mix well;
[0033] (3) Add 10g of β-cyclodextrin to the mixed solution of the above step (2) to obtain a mixed slurry;
[0034] (4) Add the mixed slurry obtained in step (3) into the coating machine, dip the gauze overcoating slurry, apply 150 grams of slurry per square meter of gauze, and fold it after coating to obtain a hemostatic and detoxifying solution. Smelly dressing.
Embodiment 3
[0036] (1) 890g vaseline and 89g liquid paraffin are mixed evenly, and set aside;
[0037] (2) Take 100g of the above-mentioned mixed solution obtained in step (1), add 10g of bismuth tribromophenate to it, and mix well;
[0038] (3) Add 10g of gamma-cyclodextrin to the mixed solution of the above step (2) to obtain a mixed slurry;
[0039] (4) Add the mixed slurry obtained in step (3) into the coating machine, dip the gauze overcoating slurry, apply 150 grams of slurry per square meter of gauze, and fold it after coating to obtain a hemostatic and detoxifying solution. Smelly dressing.