Nano cerium peroxide catalyst and method for catalyzing TMB color development by using same
A technology of cerium peroxide and catalyst, applied in the field of analysis and detection, to achieve the effect of overcoming dependence, short cycle and mild reaction conditions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] A kind of nano cerium peroxide catalyst, its preparation method comprises the steps:
[0031] Under the action of stirring, dissolve 1.012 g of cerium sulfate tetrahydrate and 5 g of polyvinylpyrrolidone in 250 mL of deionized water, then add 0.3 g of sodium hydroxide and 5 mL of 30% hydrogen peroxide in sequence, and react for 30 minutes to obtain the red Brown nanometer cerium peroxide catalyst.
[0032] The nano cerium peroxide catalyst obtained in this example is used to catalyze the color development of TMB, and the specific steps include: adding 1.6 mg nano cerium peroxide to 8 mL of phosphate buffer solution with different pH values containing 0.125 mg / mL TMB (pH is respectively 7.4, 7.0, 6.4, 6.0, 5.4), form a mixed solution I, incubate at room temperature for 5 minutes to obtain a solution system II, and use a UV spectrophotometer (scanning at 652 nm) to observe the absorbance change of the obtained solution system II.
[0033] figure 1 It is the X-ray diff...
PUM
Property | Measurement | Unit |
---|---|---|
concentration | aaaaa | aaaaa |
concentration | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com