Wood fiber manufacturing method

A production method, wood fiber technology, applied in wood treatment, impregnated wood, manufacturing tools, etc., can solve the problems of low drying efficiency, high energy consumption, large equipment area, etc.

Pending Publication Date: 2020-05-12
TAIZHOU UNIV
View PDF0 Cites 2 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0005] Judging from the current situation and development trend of fiber drying equipment at home and abroad, whether it is the traditional wood fiber drying technology with high energy consumption and low drying efficiency, or the new drying technology that has developed to a certain extent within their respective scope of application, it has not yet been completely solved. Key technical issues such as large equipment area, high energy consumption, and poor dispersion of dry materials

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment Construction

[0018] The present invention will be further described below:

[0019] The present invention comprises the following steps:

[0020] S1: Choose corn stalk husk and fast-growing poplar as raw materials;

[0021] S2: Cut the raw material into strips with a thickness of 2cm and a width of 2cm, and the length should be suitable for the range of the hydraulic press;

[0022] S3: soak the cut wood strips in the wood soaking solution for 6-10 hours;

[0023] S4: drying the flattened and soaked wood with hot air;

[0024] S5: The air-dried raw materials are pulverized in a fiber pulverizer respectively, rubbed, rolled and sieved through the bottom screen under the action of high-strength friction, shear and impact forces of the fiber pulverizer, obtained according to different specifications A sieve can obtain wood fibers with an aspect ratio of 3-7.

[0025] Further, the wood soaking solution is composed of polyethylene glycol, citric acid, fatty alcohol polyoxyethylene ether, bo...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a wood fiber manufacturing method. The wood fiber manufacturing method comprises the following steps of selecting corn stalk husk and fast-growing poplar as raw materials; cutting the raw materials into strips with the thickness of 2 cm and the width of 2 cm and the appropriate length in the range adaptive to a hydraulic machine; soaking the cut wood strips in a wood soaking solution for 6 to 10 hours; drying flattened and soaked wood by adopting hot air; and crushing the dried raw materials in a fiber crushing machine and screening through bottom screens by rubbing androlling under the actions of high-strength friction force, shear force and impact force of the fiber crushing machine, so that the wood fibers with the length-to-diameter ratio of 3 to 7 can be obtained according to the screens with different specifications. According to the wood fiber manufacturing method, the corn stalk husk and the fast-growing poplar are selected as the raw materials; dryingcharacteristics of the wood fibers and a process control method are provided; wood can be effectively softened by adopting the wood soaking solution provided by the invention, so that the wood fibersare kept intact; high-quality wood fibers are prepared by matching optimal process parameters; and the wood fiber manufacturing method is energy-saving and environment-friendly, and has popularizationand application value.

Description

technical field [0001] The invention relates to the technical field of wood processing, in particular to a wood fiber production method. Background technique [0002] Wood fiber drying is the link that consumes the most energy in the production process of wood products. The energy consumption of wood fiber drying equipment accounts for about 45%-60% of the total energy consumption of product production, and the drying efficiency is low. Traditional fiber drying methods will be gradually eliminated or transformed, so exploring a low-energy, fast, and environmentally-friendly drying technology that makes wood fibers highly dispersed meets the requirements of efficient utilization of biomass resources and the development of low-carbon circular economy today. [0003] The traditional methods of wood fiber drying include hot air circulation oven drying, drum drying, pipeline air drying, infrared radiation drying and microwave drying. Hot air circulation oven drying is a wood fib...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): B27L11/08B27K3/02B27K3/52B27K3/36B27K3/16B27K3/00B27K5/06B27K5/04
CPCB27L11/08B27K3/02B27K3/52B27K3/36B27K3/163B27K3/005B27K5/06B27K5/04
Inventor 夏兴华陈峰许楗昀林霜龚璐王海亚
Owner TAIZHOU UNIV
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products