Wooden mold of square box structure
A technology of wooden molds and square boxes, which is applied in the direction of wood processing equipment, the joining of wooden veneers, chemical instruments and methods, etc., can solve the problems of multi-wood, wooden mold cracking, consumption, etc., achieve high precision, and are not easy to absorb water Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] as attached figure 1 As shown, a wooden formwork with a square box structure whose working surface is the inner wall surface, the solid wood strips 1 are spliced and fixed together to enclose a quadrilateral skeleton, and the multilayer boards 2 are fixed on the skeleton to form an openable and closed square box. Laminate 2 is used as the working surface of the box, and plastic foam 3 is filled between the laminate 2 and the solid wood strip 1 . The solid wood strips 1 and the solid wood strips 1 can be connected with nails or falcons. The multi-layer board 2 and the solid wood strip 1 can be fixed by nails, or can be directly clamped together, and the multi-layer board 2 and the multi-layer board 2 can be connected by nails or glued together.
Embodiment 2
[0035] as attached figure 2 As shown, a wooden formwork with a square box structure whose working surface is the outer wall surface, the solid wood strips 1 are fixed together to form a cross-shaped skeleton, the multilayer boards 2 are fixed on the four edges of the skeleton, and the multilayer boards 2 surround a It is a square box, and the outer wall surface of the box is a working surface, and foam plastic 3 is filled between the solid wood strip 1 and the multi-layer board 2 .
Embodiment 3
[0037] A kind of preparation method of multi-layer board, see attached image 3 , including a brass board 202 and a wood board 201 , the wood board 201 is pasted on both sides of the brass board 202 .
[0038] The preparation method is as follows,
[0039] S1: Soak a 10mm thick wooden board and a 3mm thick brass plate in 0.1mol / L sodium hydroxide solution for 5 minutes, then soak in 0.1mol / L dilute hydrochloric acid solution for 5 minutes, and then place Ultrasonic treatment in deionized water for 20 minutes, and finally blow dry with airflow at 45°C to 50°C; the volume ratio of oxygen in the airflow is 15%, the proportion of nitrogen is 82%, and the humidity of the airflow is 35%, and the flow rate of the gas is 7m / s ;
[0040] S2: Dissolve 1 part of silica nanoparticles evenly in 300 parts of water-based glue, maintain the temperature of the water-based glue at 55°C, then put the wooden board 201 and the brass board 202 in the water-based glue, and make the wooden board on...
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com