A technology of pantoic acid and pantolactone, which is applied in carboxylate preparation, organic chemical methods, organic chemistry, etc., can solve the problems of low content, research, and inability to judge the application direction, and achieve high purity and less impurities , The preparation method is simple and easy to implement
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] A kind of preparation method of calcium D-pantoate is as follows:
[0030] (1) In a clean 500mL single-necked bottle, add 100g of deionized water successively, and the specific rotation is +46°D-pantolactone 50g, stir and dissolve, then add 114g of 25wt% calcium hydroxide aqueous solution dropwise, at 60°C React for 1h to obtain a mixed solution containing calcium D-pantoate;
[0031] (2) The mixed solution containing D-calcium pantoate is cooled down to -5° C. for crystallization after stirring, then filtered and dried to obtain D-calcium pantoate.
Embodiment 2
[0033] A kind of preparation method of calcium D-pantoate is as follows:
[0034] (1) In a clean 500mL single-necked bottle, add 100g of deionized water successively, and the specific rotation is +46 ° D-pantoate lactone 50g, stir and dissolve, then add 114g of 25wt% calcium hydroxide aqueous solution dropwise, at 80°C React for 1h to obtain a mixed solution containing calcium D-pantoate;
[0035] (2) The mixed solution containing D-calcium pantoate is cooled down to -5° C. for crystallization after stirring, then filtered and dried to obtain D-calcium pantoate.
Embodiment 3
[0037] A kind of preparation method of calcium D-pantoate is as follows:
[0038] (1) In a clean 500mL single-necked bottle, add 100g of deionized water successively, and the specific rotation is +46 ° D-pantoate lactone 50g, stir and dissolve, then add 190g of 15wt% calcium hydroxide aqueous solution dropwise, at 80°C React for 3 hours to obtain a mixed solution containing calcium D-pantoate;
[0039] (2) The mixed solution containing D-calcium pantoate was cooled down to -5° C. for 6 hours to crystallize after stirring, then filtered and dried to obtain D-calcium pantoate.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com