Embodiment 1
[0026] Provide a kind of preparation method of deep eutectic solvent cationic collector, concrete steps are:
[0027] Weigh methyltrioctylammonium chloride and lactic acid in a molar ratio of 1:2, mix and stir magnetically at 35°C in a water bath until a colorless, uniform and clear deep eutectic solvent is obtained.
[0028] The infrared spectrum of the prepared deep eutectic solvent cationic collector is shown in figure 1 . Among them, methyl trioctyl ammonium chloride is respectively in 2924.98cm -1 、2885.82cm -1 、1461.78cm -1 and 1374.11cm -1 CH appears at 3 , CH 2 and the peaks of the symmetric, antisymmetric and bending vibrations of CH, C-N are characterized at 1634.39cm -1 、1046.72cm -1 and 726.24cm -1 at the peak. Lactic acid at 3355.54cm -1 and 1731.41cm -1 The peaks at correspond to the vibrations of C-OH and C=O, respectively, while the rest of the absorption peaks are related to the vibrations of C-OH and the structure of CH. Compared with single comp...
Embodiment 2
[0032] Provide a kind of preparation method of deep eutectic solvent cationic collector, concrete steps are as follows:
[0033] Weigh methyl trioctyl ammonium chloride and lactic acid at a molar ratio of 1:4, mix and stir magnetically at 35°C in a water bath until a colorless, uniform and clear deep eutectic solvent is obtained.
[0034] The deep eutectic solvent cation collector prepared above was used for reverse flotation desiliconization of artificial mixed iron ore, and the specific steps were the same as in Example 1.
[0035] After the flotation, the foam product (iron concentrate) and the product in the tank (iron tailings) were dried and weighed to calculate the recovery rate, and the iron concentrate product grade was 65.86%, and the recovery rate was 83.88%.
Embodiment 3
[0037] Provide a kind of preparation method of deep eutectic solvent cationic collector, concrete steps are as follows:
[0038] Weigh methyltrioctylammonium chloride and lactic acid at a molar ratio of 1:6, mix them and stir them magnetically at 35°C in a water bath until a colorless, uniform and clear deep eutectic solvent is obtained.
[0039] The deep eutectic solvent cation collector prepared above was used for reverse flotation desiliconization of artificial mixed iron ore, and the specific steps were the same as in Example 1.
[0040] After the flotation, the foam product (iron concentrate) and the product in the tank (iron tailings) were dried and weighed to calculate the recovery rate, and the iron concentrate product grade was 64.59%, and the recovery rate was 82.68%.