Carbonate reservoir microcosmic model, and preparation method and application thereof

A carbonate rock reservoir and microscopic model technology, applied in teaching models, educational appliances, instruments, etc., can solve problems such as affecting experimental results, affecting the contact angle between water and calcium carbonate surface, etc., and achieves accelerated speed and simple preparation method. Fast, pressure-resistant effects

Active Publication Date: 2021-04-02
CHINA UNIV OF PETROLEUM (BEIJING) +1
View PDF17 Cites 2 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

In the process of water injection development, it will affect the contact angle between water and calcium carbonate surface, thus affecting the experimental results

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Carbonate reservoir microcosmic model, and preparation method and application thereof
  • Carbonate reservoir microcosmic model, and preparation method and application thereof
  • Carbonate reservoir microcosmic model, and preparation method and application thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0055] The present embodiment provides a method for preparing a carbonate reservoir microscopic model, which includes the following steps:

[0056] 1. Calcite crystal cutting:

[0057] (1) Crystal slicing: Cut the calcite crystal into crystal slices with a thickness of 3-4 mm using a thin saw or a precision wire cutter.

[0058] (2) Grinding of crystal slices: Use digitally controlled precision machining lathes to grind the crystal slices to ensure that both sides are smooth and flat, in preparation for subsequent uniform etching and bonding.

[0059] (3) Cleaning of crystal slices: Rinse the calcite crystal slices with ethanol and ether respectively, then rinse the surface with deionized water for 3 minutes, and place them in an oven at 105°C for 2 hours to dry after rinsing.

[0060] 2. Preparation of protective coating:

[0061] (1) Production of wax coating: put the crystal sheet into a beaker heated to 160°C filled with molten beeswax and soak for 1 min, then take it ou...

Embodiment 2

[0076] Adopt the method for preparing the microscopic model of carbonate rock reservoir in embodiment 1, design the model pattern channel to be many regular 2.5D hexagonal channels of etching, the inlet and outlet channels on both sides are parallel straight channels, and the length is 100mm. The channel width is 100 μm (such as figure 1 Shown), according to the method of embodiment 1, preparation obtains the microscopic model of carbonate rock reservoir, this model is used in the research of water injection development of carbonate rock, and concrete operation is as follows:

[0077] The Sudan 4 red-dyed kerosene was injected from the inlet and outlet channels on both sides until the model was fully saturated with kerosene, and then the inlet and outlet channels on both sides were simultaneously injected with kerosene and EOR liquid system with enhanced water injection effect at the same pressure and constant pressure. The pressure on both sides is the same, and the pressure ...

Embodiment 3

[0080] Adopt the method for preparing the microscopic model of the carbonate rock reservoir in Example 1, design the channel of the model pattern to be a straight channel, the width of the straight channel is inconsistent, and the intervals of 30 μm and 120 μm are arranged (in order to be consistent with the occurrence of remaining oil in the water injection process, by observing the remaining oil The contact angle between oil and wall surface and water, to judge the effect of enhanced oil recovery liquid system with enhanced water injection effect), prepare and obtain the microscopic model of carbonate rock reservoir according to the method of Example 1, and use this model to judge the effect of enhanced oil recovery liquid system The research on the effect of the enhanced oil recovery liquid system of the water injection effect, the specific operation is as follows:

[0081] Inject Sudan 4 red-dyed kerosene from the injection port of the model until the model is fully saturat...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention provides a carbonate reservoir microcosmic model and a preparation method and application thereof. The model preparation method comprises the following steps: cutting calcite crystals into crystal pieces; soaking crystal wafer in molten beewax to form a wax coating on the surface; adopting a carbon dioxide laser to remove the wax coating on the front surface of the corresponding crystal wafer according to the mapping shape of the target pattern channel on the front surface of the crystal wafer, and completing mapping re-etching of the target pattern channel; immersing the front surface of the crystal wafer into hydrochloric acid upwards and carrying out ultrasonic oscillation to etch the exposed channel pattern of the wax coating; drilling an inlet and outlet channel for communicating the etched channel with the outside; and covering the front surface of the crystal plate with a glass cover plate and an adhesive to bond the crystal plate, then cleaning the channel, and wetting and modifying the channel to obtain the carbonate reservoir microcosmic model. The carbonate reservoir microcosmic model preparation method is simple and rapid, the model bearing capacity is extremely high, and the carbonate reservoir microcosmic model preparation method can be used for researching the influence of wettability on the effect of improving the recovery ratio through carbonate water injection development.

Description

technical field [0001] The invention belongs to the technical field of pore-scale fluid flow in the process of oil and gas development, and relates to a carbonate reservoir microscopic model, its preparation method and application. Background technique [0002] At present, more than 99% of the oil and gas reserves discovered in the world are concentrated in sedimentary rocks, and the sedimentary rocks are dominated by carbonate rock and sandstone reservoirs. Among them, the oil and gas reserves in carbonate rock reservoirs account for a huge proportion, oil accounts for more than 60% of the global reserves, and natural gas accounts for more than 40% of the global reserves. However, carbonate oil and gas reservoirs are affected by diagenesis, have strong heterogeneity, poor pore connectivity, and low permeability. active agent) to increase the productivity of oil and gas wells. [0003] In the research of water injection development, the surfactant adsorbs on the oil-wet su...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): G09B23/40
CPCG09B23/40
Inventor 梁天博周福建苏航于馥玮李源李俊键左洁杨凯曲鸿雁姚二冬李奔胡晓东
Owner CHINA UNIV OF PETROLEUM (BEIJING)
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products