A kind of amphoteric synthetic fatliquor and its preparation method and application
A fatliquor, amphoteric technology, applied in the field of amphoteric synthetic fatliquor and its preparation, can solve the problems of low binding force, low utilization rate, increased cost, etc. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0042] The present invention also provides the preparation method of the amphoteric synthetic fatliquor described in the above technical scheme, comprising the following steps:
[0043] Mixing hydroxyorganic amine and maleic anhydride, carry out amidation reaction to obtain amidation product;
[0044] Mixing the amidated product and an acidic catalyst, and carrying out an esterification reaction to obtain an esterified product;
[0045] Mixing the esterified product with a long-chain vinyl compound and an initiator, and carrying out a vinyl polymerization reaction to obtain a polymerized product;
[0046] The polymerized product is mixed with water, pre-emulsified, and the obtained pre-emulsified system is saponified to obtain an amphoteric synthetic fatliquor.
[0047] In the present invention, preferably, before preparing the amphoteric synthetic fatliquor, all raw material components except water are dried until moisture-free. In a specific embodiment of the present inventi...
Embodiment 1
[0058] Dry all materials except water until moisture-free;
[0059] In parts by weight, 150 parts of N,N-bis(2-hydroxyethyl)ethylenediamine and 98 parts of maleic anhydride were added to the reactor, heated to 40°C, and subjected to amidation reaction for 3 hours to obtain amidation products;
[0060] Add solid acid catalyst B to the amidation product 2 O 3 -Al 2 O 3 10 parts, carry out esterification reaction at 150 ℃ for 6 hours to obtain esterification product;
[0061] To the esterified product, 22 parts of carboxymethyl octadecyl methyl diallyl ammonium chloride, 300 parts of octadecyl acrylate and 10 parts of benzoyl peroxide were added, and vinyl chloride was carried out at 90° C. The polymerization reaction was carried out for 4 hours, 1000 parts of distilled water was added, the mixture was stirred at 2000 rpm for 1 hour, and the pH value was adjusted to 7.0 with a 30% sodium hydroxide solution to obtain an amphoteric synthetic fatliquor.
Embodiment 2
[0063] Dry all materials except water until moisture-free;
[0064] In parts by weight, 236 parts of N,N,N',N'-tetrahydroxyethylethylenediamine and 300 parts of maleic anhydride were added to the reactor, heated to 80°C, and carried out amidation reaction for 2 hours , to obtain an amidated product;
[0065] Add 12 parts of p-toluenesulfonic acid to the amidation product, and carry out an esterification reaction at 120° C. for 6 hours to obtain an esterified product;
[0066] Add 295 parts of hexadecyl acrylate and 10 parts of azobisisobutyronitrile to the esterified product, carry out the first vinyl polymerization reaction at 110 ° C for 3 hours, and then add 100 parts of tetraallyl ammonium chloride , add 10 parts of ammonium persulfate, carry out the second vinyl polymerization reaction at 110 ° C for 3 hours, add 2000 parts of distilled water, stir at a speed of 3000 rpm for 1 hour, adjust the pH value to 6.8 with a 30% sodium hydroxide solution , to obtain the amphoter...