[0039] According to one embodiment of the present invention, the rubber composition comprises the following components in parts by weight: 100 parts in total of natural rubber, styrene-butadiene rubber, and butadiene rubber; 5 parts of functional additives; 60 parts of reinforcing agent 4 parts of anti-aging agent; 4 parts of vulcanizing agent; 2 parts of accelerator; 4 parts of zinc oxide; 3 parts of stearic acid; 0.5 parts of anti-scorch agent; 2 parts of silane coupling agent; 10 parts of plasticizer.
[0040] figure 1 A flow chart of a method for preparing a rubber composition used for snow groomer tracks is shown.
[0041] Such as figure 1 As shown, the present invention also provides a method for preparing a rubber composition used for snow groomer tracks, including, the first step S1, preparing a functional auxiliary: the functional auxiliary uses natural rubber as a raw material, by The click chemical reaction is obtained by grafting functional small molecular compou...
Embodiment 1
[0045] Add 10 parts of natural rubber, 20 parts of cis-butadiene rubber, 70 parts of styrene-butadiene rubber and 2 parts of functional additives into the internal mixer for mastication for 1 min; add 4 parts of anti-aging agent, 4 parts of zinc oxide, and 3 parts of stearic acid , 0.5 parts of anti-scorch agent were added into the internal mixer and mixed for 1.5 minutes; 2 parts of silane coupling agent, 60 parts of reinforcing agent and 10 parts of plasticizer were added into the internal mixer, and mixed for 3 minutes to obtain a masterbatch ;Put a piece of master batch into the open mill, add 4 parts of vulcanizing agent and 2 parts of accelerator, fully mix evenly, and get the mixed rubber; then, stop for 16h, vulcanize at 150°C for 30min, and obtain rubber Composition, performance test see Table 1.
Embodiment 2
[0047] Add 10 parts of natural rubber, 20 parts of butadiene rubber, 70 parts of styrene-butadiene rubber and 5 parts of functional additives into the internal mixer for mastication for 1 min; add 4 parts of anti-aging agent, 4 parts of zinc oxide, and 3 parts of stearic acid , 0.5 parts of anti-scorch agent were added into the internal mixer and mixed for 1.5 minutes; 2 parts of silane coupling agent, 60 parts of reinforcing agent and 10 parts of plasticizer were added into the internal mixer, and mixed for 3 minutes to obtain a masterbatch ;Put a piece of master batch into the open mill, add 4 parts of vulcanizing agent and 2 parts of accelerator, fully mix evenly, and get the mixed rubber; then, stop for 16h, vulcanize at 150°C for 30min, and obtain rubber Composition, performance test see Table 1.