Washable environment-friendly stiffening agent and preparation method thereof
A stiffening agent and water-resistant technology, applied in the direction of wear-resistant fibers, light-resistant fibers, fiber types, etc., can solve the problems of affecting the living environment, endangering health, high chemical composition, etc., to achieve improved dispersion effect, good adhesion effect, The effect of high thermal conductivity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0039] The preparation method comprises the following steps:
[0040] S1. Put silane coupling agent and nano-silicon carbide into a ball mill in parts by mass, and perform ball milling modification under nitrogen atmosphere; the diameter of the balls is 0.5-20mm; the mass ratio of raw materials to balls is 1:(10-1000) ;
[0041] S2, put polyvinyl alcohol and starch into the ball mill, and mix the ball mill for 1-4h;
[0042] S3. Put in water and emulsifier, heat up to 80-100°C and adjust the pH value to 4-6, and ball mill for 0.5-1h;
[0043] S4, put in initiator and antibacterial agent, cool down to 40-60°C, and ball mill for 1-2h;
[0044] S5. Adjust the pH to 8-9, and ball mill for 0.5-1 hour to prepare the stiffening agent.
Embodiment 1-4
[0046]
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle diameter | aaaaa | aaaaa |