Special anti-bursting cover oil for ceramic stained paper, production process of special anti-bursting cover oil and ceramic stained paper
A production process and technology of cover oil, applied in special paper, papermaking, paper and other directions, can solve the problems of ceramic popping, explosion-proof cover oil reducing the rate of ceramic popping, reducing the rate of ceramic popping, etc., and achieve good plasticizing properties. , avoid popping defects, increase the effect of easy decomposition speed
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0037] Further illustrate, in step (4), the preparation method of epoxy adipate polyester comprises the following steps:
[0038] a. Mix 8-12 parts of adipic acid polyester, 0.5-1.5 parts of formic acid and 8-12 parts of acetone in parts by mass, and heat up to 60-70°C to obtain a mixed solution;
[0039] b. Add 1.5-3 parts of hydrogen peroxide and 1.5-3 parts of formic acid to the mixture, keep the temperature at 60-70°C, and keep it warm for 3-5 hours;
[0040] c, feed chlorine gas into the mixed solution in step b, and irradiate for 2-4h under ultraviolet light;
[0041] d. Nitrogen gas is introduced to replace chlorine gas, and the epoxy-based adipate polyester plasticizer is obtained through static stratification, water washing and dehydration in sequence.
[0042]It is worth noting that, using the above method, epoxy groups are grafted on the adipate polyester, thereby preparing the epoxy adipate polyester, so that the epoxy adipate polyester has the characteristics of ...
Embodiment 1
[0055] A kind of production technology of explosion-proof decal cover oil special for ceramic decal paper, comprises the following steps:
[0056] (1) According to the number of parts by mass, 30 parts of solvent and 0.1 part of defoamer were mixed and stirred for 20min, and the stirring speed was 1500r / min to obtain mixed material A; wherein, the flux was a mixture of trimethylbenzene and tetramethylbenzene, and the defoamer was organosiloxane;
[0057] (2) Add 40 parts of thermoplastic acrylic resin to the mixture A, stir for 50 minutes, and the stirring speed is 1500r / min, to obtain the mixture B; wherein, the thermoplastic acrylic resin is a methacrylic acid polymer;
[0058] (3) Add 1 part of thickening thixotropic agent to mixed material B, stir for 30min, stirring speed is 1500r / min, obtain mixed material C; wherein, thickening thixotropic agent is fatty acid amide thixotropic agent;
[0059] (4) Pass cooling water into the mixed material C until the temperature of the...
Embodiment 2
[0066] The production process of the special anti-explosion cover oil for ceramic decal paper in this embodiment is the same as that of Example 1, the difference is that the raw material formula of the anti-explosion cover oil in this embodiment is different from that of Example 1, and in parts by mass, this embodiment The raw materials of the explosion-proof cover oil in the example include 50 parts of thermoplastic acrylic resin, 0.3 parts of defoamer, 3 parts of thickening thixotropic agent, 40 parts of solvent, and 5 parts of polymer polyester plasticizer. The raw material formula of this embodiment is adopted And the production process, the anti-explosion flower cover oil specially used for ceramic decal paper is prepared.